Stoody 970-G is a non-chromium bearing hardfacing welding wire that provides a deposit with wear resistance and hardness equal to or better than that of conventional chromium carbide. Specially formulated to eliminate chromium in the wire, Stoody 970-G provides outstanding wear resistance. With no chromium in the welding wire, the emission of hexavalent chromium during welding is reduced or completely eliminated (depending on the chromium content of the base metal or the pre-existing weld deposit). Stoody 970-G provides a wear-resistant overlay for applications where hexavalent chromium in welding fumes cannot be reduced by work practice controls.

Where To Buy


Features

  • Non-chromium bearing
  • Excellent abrasion resistance
  • Low to medium impact resistance


Specifications


Typical Tensile Properties

98% Ar - 2% O2
Hardness (HRC)
67-71 HRC

Typical Weld Metal Analysis %

OtherCFe
6.5 %1.0 %BAL %

x

Typical Tensile Properties

98% Ar - 2% O2
Hardness (HRC)
67-71 HRC

Typical Weld Metal Analysis %

OtherCFe
6.5 %1.0 %BAL %

x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : Stoody 970-G
1/16 in / 1.6 mm Stoody 970-G Hardfacing Wire 50# Poly Pak 11994700 Buy Local
1/16 in / 1.6 mm Stoody 970-G Hardfacing Wire 33# Wire Basket 11996200 Buy Local
0.045 in / 1.2 mm Stoody 970-G Hardfacing Wire 33# Wire Basket 11994800 Buy Local
x
×

Find the Closest Distributor


x

Find the Closest Distributor

x

x

Loading..