Typical Tensile Properties

98% Ar - 2% O2
Hardness (HRC)
56-60 HRC

Typical Weld Metal Analysis

OtherCCrFe
4.0 %0.5 %6.0 %BAL %

x

Typical Tensile Properties

98% Ar - 2% O2
Hardness (HRC)
56-60 HRC

Typical Weld Metal Analysis

OtherCCrFe
4.0 %0.5 %6.0 %BAL %