Stoody

Stoody 964-APG

Stoody 964-APG

Stoody 964 AP-G is a gas shielded flux cored general purpose hardfacing wire. Deposits from this all-position wire provide exceptional wear resisteance and high hardness. On Series 300 stainless and manganese steels, deposits are crack free. Other base metals should be preheated and post-heated appropriately. Stoody 964AP-G provides improved weldability over chromium carbide and many other tool steel welding wires. Use 964 AP-G where cross checking is undesirable.

Where To Buy


Features

  • Gas shielded flux cored
  • All position
  • Excellent wear resistance
  • High hardness
  • Crack free on Series 300 stainless and manganese steels
  • Little or no cross checking
  • Improved weldability over chromium carbides and tool steel welding wires


Specifications


Typical Tensile Properties

75% Ar - 25% CO2
Hardness (HRC)
58-64 HRC

Typical Weld Metal Analysis %

OtherCCrFe
6.5 %1.0 %8.0 %BAL %

x

Typical Tensile Properties

75% Ar - 25% CO2
Hardness (HRC)
58-64 HRC

Typical Weld Metal Analysis %

OtherCCrFe
6.5 %1.0 %8.0 %BAL %