Stoody 105-G deposit is a low alloy steel developed for the rebuilding of carbon and low alloy steels parts used in applications involving metal-to-metal wear.

BUY NOW


Features

  • Multiple layers can be applied without difficulty when proper preheat and interpass temperatures are maintained.

Specifications


Typical Tensile Properties

98% Ar - 2% O2
Hardness (HRC)
41-46 HRC

Typical Weld Metal Analysis

OtherCCrFe
4.0 %0.5 %3.0 %BAL %

x

Typical Tensile Properties

98% Ar - 2% O2
Hardness (HRC)
41-46 HRC

Typical Weld Metal Analysis

OtherCCrFe
4.0 %0.5 %3.0 %BAL %