Stoody 102-G'

Stoody

Stoody 102-G

Stoody 102-G

Stoody 102 deposit has a composition and physical properties that are similar to those of H-12 tool steel. Weldability is very good and the wire can be applied out-of-position. Stoody 102 requires carbide tools for machining. It is good for hot wear applications up to 1100F.

BUY NOW


Features

  • Multiple layers can be applied without difficulty when proper preheat and interpass temperatures are maintained.

Specifications


Typical Tensile Properties

98% Ar - 2% O2
Hardness (HRC)
48-53 HRC

Typical Weld Metal Analysis

OtherCCrFe
5.0 %0.5 %8.0 %BAL %

x

Typical Tensile Properties

98% Ar - 2% O2
Hardness (HRC)
48-53 HRC

Typical Weld Metal Analysis

OtherCCrFe
5.0 %0.5 %8.0 %BAL %