This site uses cookies and other tracking technologies to provide you with our services, enhance the performance and functionality of our services, analyze the use of our products and services, and assist with our advertising and marketing efforts.

Cookie Policy   Privacy Notice

Previous Next
Stoody

Stoody 101HC-G

Stoody 101HC-G

Stoody 101HC is a high chromium-iron based alloy recommended for metal-to earth applications subject to severe abrasion and moderate impact and heat. 101HC develops a tight crosschecking pattern.

Where To Buy


Features

  • Very tight cross checking pattern
  • Good choice for applications involving severe metal-to-earth abrasion
  • Can be used in hot wear applications up to 900° F (482° C)


Specifications


Typical Tensile Properties

98% Ar - 2% O2
Hardness (HRC)
56-64 HRC

Typical Weld Metal Analysis %

OtherCCrFe
2.0 %5.0 %19.0 %BAL %

x

Typical Tensile Properties

98% Ar - 2% O2
Hardness (HRC)
56-64 HRC

Typical Weld Metal Analysis %

OtherCCrFe
2.0 %5.0 %19.0 %BAL %

x