Stoody

Stoodite 6-M

Stoodite 6-M

Stoodite 6-M is the most widely used cobalt alloy with excellent resistance to many forms of mechanical and chemical degradation over a wide temperature range. Stoodite 6-M attributes include its outstanding self mated anti-galling properties, high temperature hardness, and high resistance to cavitation erosion. Certification to AWS specification - A5.21 ERCCoCr-A

Where To Buy


Features

  • Excellent resistance to many forms of mechanical and chemical degradation over a wide temperature range
  • Outstanding self mated anti-galling properties
  • Cavitation erosion resistant
  • High temperature hardness


Specifications


Typical Tensile Properties

100% Ar
Hardness (HRC)
35-40 HRC

Typical Weld Metal Analysis %

MnMoCSiWNiCoCrFe
0.9 %0.1 %1.2 %0.6 %4.0 %0.2 %BAL %28.1 %4.0 %

Classifications: AWS A5.21; ERCCoCr-A

x

Typical Tensile Properties

100% Ar
Hardness (HRC)
35-40 HRC

Typical Weld Metal Analysis %

MnMoCSiWNiCoCrFe
0.9 %0.1 %1.2 %0.6 %4.0 %0.2 %BAL %28.1 %4.0 %

Classifications: AWS A5.21; ERCCoCr-A

x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : Stoodite 6-M
.045 in / 1.2 mm Stoodite 6-M 25lb WB-LLW 810722182045 Buy Local
1/16 in / 1.6 mm Stoodite 6-M 25lb WB-LLW 810722182062 Buy Local
x
×

Find the Closest Distributor


x

Find the Closest Distributor

x

x

Loading..