Stoodite 21-M

Stoodite 21-M offers excellent high temperature strength making it suitable for use on hot die parts. Deposits are inherently resistant to galling, cavitation erosion, and corrosion. Abrasion resistance is slightly lower but offset by outstanding impact strength at high temperatures and anti-galling properties. Certification to AWS specification - A5.21 ERCCoCr-E

Where To Buy


Features

  • High temperature hardness
  • Excellent resistance to many forms of mechanical and chemical degradation over a wide temperature range
  • Corrosion, cavitation erosion, and galling resistance


Specifications


Typical Weld Metal Analysis %

MnMoCSiWNiCoCrFe
0.9 %0.1 %1.4 %1.1 %8.3 %0.2 %BAL %27.3 %3.9 %

Classifications: AWS A5.21; ERCCoCr-B; AWS A5.21; ERCCoCr-E

x

Typical Weld Metal Analysis %

MnMoCSiWNiCoCrFe
0.9 %0.1 %1.4 %1.1 %8.3 %0.2 %BAL %27.3 %3.9 %

Classifications: AWS A5.21; ERCCoCr-B; AWS A5.21; ERCCoCr-E

x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : Stoodite 21-M
.045 in / 1.2 mm Stoodite 21-M 25lb WB-LLW 812122182045 Buy Local
1/16 in / 1.6 mm Stoodite 21-M 25lb WB-LLW 812122182062 Buy Local
.045 in / 1.2 mm Stoodite 12-M 25lb WB-LLW 11927400 Buy Local
x
×

Find the Closest Distributor


x

Find the Closest Distributor

x

x

Loading..