This site uses cookies and other tracking technologies to provide you with our services, enhance the performance and functionality of our services, analyze the use of our products and services, and assist with our advertising and marketing efforts.

Cookie Policy   Privacy Notice

Previous Next
Stoody

Stoodite 12-M

Stoodite 12-M

Stoodite 12-M is a more wear resistant cobalt alloy than 6-M thanks to a higher volume of carbides but with lower impact strength. Produces a high hardness cobalt-chromium deposit for high temperature applications with abrasive wear associated with corrosion. Provides excellent resistance to many forms of chemical and mechanical degradation, including galling. Stoodite 12-M bonds well with all weldable steels, including stainless. Certification to AWS specification - A5.21 ERCCoCr-B

Where To Buy


Features

  • Excellent resistance to many forms of mechanical and chemical degradation over a wide temperature range
  • Anti-galling properties
  • High temperature hardness


Specifications


Typical Tensile Properties

100% Ar
Hardness (HRC)
44-45 HRC

Typical Weld Metal Analysis %

MnMoCSiWNiCoCrFe
0.9 %0.1 %1.4 %1.1 %8.3 %0.2 %BAL %27.3 %3.9 %

Classifications: AWS A5.21; ERCCoCr-B

x

Typical Tensile Properties

100% Ar
Hardness (HRC)
44-45 HRC

Typical Weld Metal Analysis %

MnMoCSiWNiCoCrFe
0.9 %0.1 %1.4 %1.1 %8.3 %0.2 %BAL %27.3 %3.9 %

Classifications: AWS A5.21; ERCCoCr-B

x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : Stoodite 12-M
1/16 in / 1.6 mm Stoodite 12-M 25lb WB-LLW 811222182062 Buy Local