Stoody

Stoodite 1-M

Stoodite 1-M

Stoodite 1-M wire has the greatest volume of carbides among the cobalt-based alloys resulting in the highest hardness yet sacrificing toughness. The chromium carbide content imparts outstanding abrasive wear resistance. The manganese, silicon, and iron levels are somewhat higher than the other Stoodite wires. Certification to AWS specification - A5.21 ERCCoCr-C

Where To Buy


Features

  • High temperature hardness
  • Excellent abrasion and solid particle erosion resistance
  • Bonds well with weldable alloy steels including stainless


Specifications


Typical Tensile Properties

100% Ar
Hardness (HRC)
46-50 HRC

Typical Weld Metal Analysis %

MnMoCSiWNiCoCrFe
0.8 %0.1 %2.6 %0.2 %11.2 %0.2 %BAL %29.0 %3.6 %

Classifications: AWS A5.21; ERCCoCr-C

x

Typical Tensile Properties

100% Ar
Hardness (HRC)
46-50 HRC

Typical Weld Metal Analysis %

MnMoCSiWNiCoCrFe
0.8 %0.1 %2.6 %0.2 %11.2 %0.2 %BAL %29.0 %3.6 %

Classifications: AWS A5.21; ERCCoCr-C

x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : Stoodite 1-M
1/16 in / 1.6 mm Stoodite 1-M 25lb WB-LLW 810222182062 Buy Local
x
×

Find the Closest Distributor


x

Find the Closest Distributor

x

x

Loading..