OK Autrodur 58 G M

OK Autrodur 58 G M is a copper-coated, low-alloyed, solid GMAW wire used for hardfacing and building up highly wear-resistant layers on machinery parts like shafts, feed screws, driving rollers, cutting tools, dies and other parts subjected to heavy wear. The hardness of the weld metal becomes 50-60 HRC.

Where To Buy


Specifications


Typical Weld Metal Analysis %

wire composition
MnCSiCr
1.87 %1.04 %0.48 %1.82 %

Classifications: EN 14700; ZFe8; Wire Electrode

Alloy Type: Low alloyed (1.1 % C, 2 % Mn, 1.8 % Cr, 0.2 % Ti)
x

Typical Weld Metal Analysis %

wire composition
MnCSiCr
1.87 %1.04 %0.48 %1.82 %

Classifications: EN 14700; ZFe8; Wire Electrode

Alloy Type: Low alloyed (1.1 % C, 2 % Mn, 1.8 % Cr, 0.2 % Ti)
x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : OK Autrodur 58 G M
OK Autrodur 58 G M 1.0mm 15kg 1390107700 Buy Local
OK Autrodur 58 G M 1.2mm 15kg 1390127700 Buy Local
x
×

Find the Closest Distributor


x

Find the Closest Distributor

x

x

Loading..