OK Autrodur 56 G M

OK Autrodur 56 G M is a copper coated, low-alloyed solid GMAW wire used for hardfacing and building up highly wear-resistant layers on tools and machinery parts, driving rollers, digging tools and so on. The hardness of the weld metal becomes 50-60 HRC.

Where To Buy


Specifications


Typical Weld Metal Analysis %

wire composition
MnCSiCr
0.4 %0.44 %3.02 %9.24 %

Classifications: EN 14700; Fe8; Wire Electrode

Alloy Type: Low alloyed (0.45 % C, 3 % Si, 9 % Cr)
x

Typical Weld Metal Analysis %

wire composition
MnCSiCr
0.4 %0.44 %3.02 %9.24 %

Classifications: EN 14700; Fe8; Wire Electrode

Alloy Type: Low alloyed (0.45 % C, 3 % Si, 9 % Cr)
x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : OK Autrodur 56 G M
OK Autrodur 56 G M 1.2mm 250kg 1391129320 Buy Local
OK Autrodur 56 G M 1.0mm 15kg 1391107700 Buy Local
OK Autrodur 56 G M 1.2mm 15kg 1391127700 Buy Local
OK Autrodur 56 G M 1.6mm 15kg 1391167700 Buy Local
x
×

Find the Closest Distributor


x

Find the Closest Distributor

x

x

Loading..