OK Autrodur 38 G M

OK Autrodur 38 G M is a copper-coated, low-alloyed, solid GMAW wire used for hardfacing and building up, producing a wear-resistant weld metal with a hardness of between 35-40 HRC. It is used for the repair and maintenance of tracks, rails, wheels, rolls, rail crossings, shafts, shovel teeth and other parts on digging machines, tools like dies and so on.

Where To Buy


Specifications


Typical Weld Metal Analysis %

wire composition
MnCTiSiCr
1.92 %0.69 %0.2 %0.49 %1.00 %

Classifications: EN 14700; Fe2; Wire Electrode

Alloy Type: Low alloyed (0.7 C, 2 % Mn, 1 % Cr, 0.2 % Ti)
x

Typical Weld Metal Analysis %

wire composition
MnCTiSiCr
1.92 %0.69 %0.2 %0.49 %1.00 %

Classifications: EN 14700; Fe2; Wire Electrode

Alloy Type: Low alloyed (0.7 C, 2 % Mn, 1 % Cr, 0.2 % Ti)
x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : OK Autrodur 38 G M
OK Autrodur 38 G M 1.0mm 15kg 1389107700 Buy Local
OK Autrodur 38 G M 1.2mm 15kg 1389127700 Buy Local
x
×

Find the Closest Distributor


x

Find the Closest Distributor

x

x

Loading..