Stoody Super Build Up deposit is a low alloy steel that can be used both as a build-up and hardfacing material because it has good compressive strength and hardness.

BUY NOW


Features

  • It is not intended to be used as an underbase for subsequent hardfacing. It can be used on carbon and low alloy steels, but not on manganese steels or cast iron.

Typical Tensile Properties

Deposition Data

Current Deposition Type Diameter TTW Dist. Voltage
140-260 A Full Range 1.6 mm (1/16 in.) 13-25 mm (1/2-1 in.) 23-26 V
200-350 A Full Range 2.4 mm (3/32 in.) 19-32 mm (3/4-1 1/4 in.) 24-28 V
350-450 A Full Range 2.8 mm (7/64 in.) 32-38 mm (1 1/4-1 1/2 in.) 26-28 V

Typical Weld Metal Analysis %

C Cr Fe Other
0.5 % 2.0 % BAL % 2.5 %