Stoody Super Build Up deposit is a low alloy steel that can be used both as a build-up and hardfacing material because it has good compressive strength and hardness.

BUY NOW


Features

  • It is not intended to be used as an underbase for subsequent hardfacing.
  • It can be used on carbon and low alloy steels, but not on manganese steels or cast iron.


Typical Tensile Properties

Shielding Gas
98% Ar - 2% O2

Deposition Data

Current 120-220 A
Deposition Type 3
Diameter .045 in.
Diameter 1.2 mm
Shielding Gas 98% Ar - 2% CO2
TTW Dist. 1/2-3/4 in.
TTW Dist. 13-19 mm
Voltage 18-24 V

Typical Weld Metal Analysis %

C Cr Fe Other
0.5 % 2.0 % BAL % 2.5 %