Stoody CP-2000 is designed to produce a high concentration of uniformly distributed small primary chromium carbides in an austenitic matrix. The formulation is optimized for superior weldability in single and multiple layer applications. CP-2000 exhibits improved wear resistance and toughness over conventional chromium carbide alloys.

BUY NOW


Features

  • Superior weldability in single and multiple layer applications.
  • Alloy exhibits improved wear resistance and toughness over conventional chromium carbine alloys.
  • Can be utilized in hot wear applications up to 900°F (482°C)


Typical Weld Metal Analysis %

Typical Tensile Properties

Deposition Data

Current Deposition Type Diameter TTW Dist. Voltage
450-650 A Full Range 3.2 mm(1/8 in.) 32-38 mm(1 1/4-1 1/2 in.) 29-33 V
175-225 A Full Range 1.2 mm(.045 in.) 13-19 mm(1/2-3/4 in.) 22-26 V
200-250 A Full Range 1.6 mm(1/16 in.) 19-25 mm(3/4-1 in.) 24-28 V
250-300 A Full Range 2.0 mm(5/64 in.) 32-38 mm(1 1/4-1 1/2 in.) 25-28 V
400-650 A Full Range 2.8 mm(7/64 in.) 32-38 mm(1 1/4-1 1/2 in.) 24-26 V
400-650 A Full Range 2.8 mm(7/64 in.) 32-38 mm(1 1/4-1 1/2 in.) 28-32 V