Stoody C-M is a nickel-based fabricated alloy cored wire for automatic/semi-automatic welding that produces a deposit resistant to high heat and corrosion accompanied by abrasion and/or impact. It is machinable but work hardens and can be applied in multiple layers.

BUY NOW


Features

Welding Procedures/Characteristics:

  • An automatic/semi-automatic wire (DECP) that can be applied in multiple layers.
    • Applications:
      • Hot Forge Dies
      • Hot Shear Blades
      • Forging Hammer Dies
      • Mill Guides
      • Shafts


Typical Tensile Properties

Shielding Gas
100% Ar

Deposition Data

Current 280-310 A
Deposition Type 3
Diameter 1/16 in.
Diameter 1.6 mm
Shielding Gas 100% Ar
TTW Dist. 1/2-3/4 in.
TTW Dist. 13-19 mm
Voltage 26-28 V
Wire Feed Speed 190-230 in./min
Wire Feed Speed 483-584 cm/min

Typical Weld Metal Analysis %

C Cr Fe Mn Mo Ni Si W
0.02 % 15.8 % 5.0 % 0.1 % 16.0 % BAL % 0.2 % 4.0 %