Stoody Build-Up-G
Stoody Build-Up is a low alloy wire with deposits exhibiting excellent compressive strength and resistance to plastic deformation. Build-up is a perfect choice for use as a buffer or build up layer to be covered by subsequent overlay hardfacing. Work hardens under impact.
Features
- Excellent compressive strength and resistance to plastic deformation
- Perfect choice for buffering and build-up layers
- Good machinability in the "as welded" condition
- Will work harden under impact
Typical Tensile Properties
Shielding Gas |
98% Ar - 2% O2 |
Deposition Data
Current | Deposition Type | Diameter | TTW Dist. | Voltage |
98% Ar - 2% CO2 | ||||
175-225 A | Full Range | 1.2 mm (.045 in.) | 13-19 mm (1/2-3/4 in.) | 18-24 V |
175-225 A | Full Range | 1.2 mm (.045 in.) | 13-25 mm (1/2-1 in.) | 18-24 V |
Typical Weld Metal Analysis %
C | Cr | Fe | Other |
0.2 % | 1.0 % | BAL % | 3.0 % |