Stoody

Stoody 965-O

The following items have been added to your list


x

Stoody 965-O is a general purpose hardfacing alloy offering a good balance of impact and abrasion resistance. Can be applied to carbon, low alloy and manganese steel. Applications would include both metal-to-metal and metal-to-earth.

BUY NOW


Features

  • Offers good balance between impact and abrasion resistance.
  • Applications would include metal-to-metal and metal-to-earth
  • Deposits are martensitic, forgeable, and not readily machinable
  • Can be applied to carbon, low alloy, and manganese steel.


Typical Tensile Properties

Deposition Data

Current 200-250 A
Deposition Type 3
Diameter 1/16 in.
Diameter 1.6 mm
TTW Dist. 3/4-1 in.
TTW Dist. 19-25 mm
Voltage 27-31 V

Typical Weld Metal Analysis %

C Cr Fe Other
0.5 % 6.0 % BAL % 3.0 %