Stoody 965-G

Stoody

Stoody 965-G

The following items have been added to your list


x

Stoody 965-G is a general purpose hardfacing alloy offering a good balance of impact and abrasion resistance. Can be applied to carbon, low alloy and manganese steel. Applications would include both metal-to-metal and metal-to-earth.

BUY NOW


Features

  • Offers good balance between impact and abrasion resistance.
  • Applications would include metal-to-metal and metal-to-earth
  • Deposits are martensitic, forgeable, and not readily machinable
  • Can be applied to carbon, low alloy, and manganese steel.


Typical Tensile Properties

Shielding Gas
98% Ar - 2% O2

Deposition Data

Current Deposition Type Diameter TTW Dist. Voltage
75% Ar - 25% CO2
80-130 A Full Range 0.9 mm (.035 in.) 13-16 mm (1/2-5/8 in.) 15-20 V
98% Ar - 2% CO2
150-200 A Full Range 1.2 mm (.045 in.) 13-19 mm (1/2-3/4 in.) 25-29 V
200-250 A Full Range 1.6 mm (1/16 in.) 19-25 mm (3/4-1 in.) 27-31 V

Typical Weld Metal Analysis %

C Cr Fe Other
0.5 % 6.0 % BAL % 4.0 %