Stoody 965 AP-G
Stoody 965 AP-G offers a good balance of impact and abrasion resistance and has a smooth semi-spray transfer. Stoody 965 AP-G can be applied to carbon, low alloy and manganese steels in metal-to-metal as well as metal-to-earth applications.
Features
- Offers good balance between impact and abrasion resistance.
- Applications would include metal-to-metal and metal-to-earth
- Deposits are forgeable, but not readily machinable
- Can be applied to carbon, low alloy, and manganese steel.
Typical Tensile Properties
Shielding Gas |
75% Ar - 25% CO2 |
Deposition Data
Current | Deposition Type | Diameter | TTW Dist. | Voltage | Wire Feed Speed |
75% Ar - 25% CO2 | |||||
140-225 A | Full Range | 1.2 mm (.045 in.) | 13-19 mm (1/2-3/4 in.) | 26-29 V | 610-1194 cm/min (240-470 in./min) |
170-275 A | Full Range | 1.6 mm (1/16 in.) | 13-19 mm (1/2-3/4 in.) | 24-30 V | 356-610 cm/min (140-240 in./min) |
Typical Weld Metal Analysis %
C | Cr | Fe | Other |
0.5 % | 8.0 % | BAL % | 2.5 % |
Part Numbers and Accessories
ESAB EQUIPMENT WARRANTIES ARE VALID ONLY WHEN PURCHASED THROUGH AN ESAB AUTHORIZED DEALERSHIP.