Stoody 600

Stoody

Stoody 600

The following items have been added to your list


x

Particularly suited for high stress applications like cement clinker crusher rolls, Stoody 600 produces a titanium carbide bearing deposit exhibiting excellent abrasion resistance as well as toughness for good impact resistance.

BUY NOW


Features

  • Titanium carbide deposit delivering excellent abrasion resistance, with toughness and good impact resistance
  • When compared to other titanium carbide alloys, Stoody 600 exhibits good operational characteristics and excellent slag removal
  • Particularly well suited to high stress applications such as cement clinker crusher rolls


Typical Weld Metal Analysis %

Typical Tensile Properties

Deposition Data

Current Deposition Type Diameter TTW Dist. Voltage
150-225 A Full Range 1.2 mm(.045 in.) 13-19 mm(1/2-3/4 in.) 22-26 V
200-300 A Full Range 1.6 mm(1/16 in.) 19-25 mm(3/4-1 in.) 22-26 V
300-400 A Full Range 2.4 mm(3/32 in.) 32-38 mm(1 1/4-1 1/2 in.) 25-27 V
400-500 A Full Range 2.8 mm(7/64 in.) 32-38 mm(1 1/4-1 1/2 in.) 26-28 V