Stoody 105-G

Stoody

Stoody 105-G

The following items have been added to your list


x

Stoody 105-G deposit is a low alloy steel developed for the rebuilding of carbon and low alloy steels parts used in applications involving metal-to-metal wear.

BUY NOW


Features

  • Multiple layers can be applied without difficulty when proper preheat and interpass temperatures are maintained.

Typical Tensile Properties

Shielding Gas
98% Ar - 2% O2

Deposition Data

Current 250-300 A
Deposition Type 3
Diameter 1/16 in.
Diameter 1.6 mm
Shielding Gas 98% Ar - 2% CO2
TTW Dist. 3/4-1 in.
TTW Dist. 19-25 mm
Voltage 25-26 V

Typical Weld Metal Analysis %

C Cr Fe Other
0.5 % 3.0 % BAL % 4.0 %
x

Part Numbers and Accessories

Select All | Select None

ESAB EQUIPMENT WARRANTIES ARE VALID ONLY WHEN PURCHASED THROUGH AN ESAB AUTHORIZED DEALERSHIP.

x
x

x

Loading..