Stoody 102-G

Stoody

Stoody 102-G

The following items have been added to your list


x

Stoody 102 deposit has a composition and physical properties that are similar to those of H-12 tool steel. Weldability is very good and the wire can be applied out-of-position. Stoody 102 requires carbide tools for machining. It is good for hot wear applications up to 1100F.

BUY NOW


Features

  • Multiple layers can be applied without difficulty when proper preheat and interpass temperatures are maintained.

Typical Weld Metal Analysis %

Typical Tensile Properties

Shielding Gas
98% Ar - 2% O2

Deposition Data

Current Deposition Type Diameter TTW Dist. Voltage
98% Ar - 2% CO2
135-185 A Full Range 1.2 mm(.045 in.) 13-25 mm(1/2-1 in.) 18-24 V
225-275 A Full Range 1.6 mm(1/16 in.) 13-25 mm(1/2-1 in.) 25-27 V