Stoodite 6-M is the most widely used cobalt alloy with excellent resistance to many forms of mechanical and chemical degradation over a wide temperature range. Stoodite 6-M attributes include its outstanding self mated anti-galling properties, high temperature hardness, and high resistance to cavitation erosion. Certification to AWS specification - A5.21 ERCCoCr-A

BUY NOW


Features

  • Excellent resistance to many forms of mechanical and chemical degradation over a wide temperature range
  • Outstanding self mated anti-galling properties
  • Cavitation erosion resistant
  • High temperature hardness


Typical Tensile Properties

Shielding Gas
100% Ar

Deposition Data

Current Deposition Type Diameter TTW Dist. Voltage
100% Ar
180-200 A Full Range 1.2 mm (.045 in.) 13-16 mm (1/2-5/8 in.) 25-27 V
280-300 A Full Range 1.6 mm (1/16 in.) 16-19 mm (5/8-3/4 in.) 26-28 V

Classifications

Grade ERCCoCr-A
Name AWS A5.21

Typical Weld Metal Analysis %

C Co Cr Fe Mn Mo Ni Si W
1.2 % BAL % 28.1 % 4.0 % 0.9 % 0.1 % 0.2 % 0.6 % 4.0 %
x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : Stoodite 6-M
810722182045 FIND A DISTRIBUTOR
810722182062 FIND A DISTRIBUTOR

ESAB EQUIPMENT WARRANTIES ARE VALID ONLY WHEN PURCHASED THROUGH AN ESAB AUTHORIZED DEALERSHIP.

x
x

x

Loading..