Arcaloy MC409Ti is a 12% Cr alloy metal cored electrode stabilized with Titanium (Ti) for arc stability and to improve corrosion resistance, increase strength at high temperatures, and promote the ferritic microstructure. Arcaloy MC409Ti produces a smooth spray-type metal transfer with very minimal spatter. It is particularly suited for welding parts with poor fit up. It was designed for welding stainless steel catalytic converters, manifolds, mufflers, and exhaust systems.

BUY NOW


Industries

  • Automotive

Welding Process

  • GMAW (MIG/MAG)
  • SAW - Submerged Arc Welding
  • MCAW - Metal Core Arc Welding

Deposition Data

Current Diameter Electrical Stickout Voltage Wire Feed Speed
200 A 1.2 mm (.045 in.) 12.7 mm 20 V 533 cm/min (210 in./min)
215 A 1.2 mm (.045 in.) 12.7 mm 21 V 584 cm/min (230 in./min)
234 A 1.2 mm (.045 in.) 12.7 mm 22 V 635 cm/min (250 in./min)
290 A 1.2 mm (.045 in.) 12.7 mm 24 V 762 cm/min (300 in./min)
323 A 1.2 mm (.045 in.) 12.7 mm 24 V 889 cm/min (350 in./min)

Classifications

Grade EC409
Name AWS A5.22

Typical Weld Metal Analysis %

Typical Weld Metal Analysis %
C Cr Mn P S Si Ti
98% Ar - 2% O2
0.02 % 11.90 % 0.72 % 0.01 % 0.01 % 0.27 % 1.00 %
x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : Arcaloy MC409Ti
ARC MC409TI 045X33#PSP 258076264 FIND A DISTRIBUTOR
ARC MC409TI 045X600#OMP 258076256 FIND A DISTRIBUTOR
ARCALOY MC409TI 045X33# SP 35SC126620 FIND A DISTRIBUTOR
ARCALOY MC409TI 045X825# OMP 35SC1294M0 FIND A DISTRIBUTOR
x
x

x

Loading..