Arcaloy MC18CrCb is an 18% Cr alloy metal cored electrode stabilized with Titanium (Ti) and Niobium (Nb). It is designed for welding Armco 18Cr-Cb HP-10TM stainless steels used in catalytic converters, manifolds, mufflers, and exhaust systems. It is also suited for welding parts with poor fit up. Arcaloy MC18CrCb produces a smooth spray-type metal transfer with very minimal spatter.

BUY NOW


Industries

  • Automotive

Welding Process

  • GMAW (MIG/MAG)
  • SAW - Submerged Arc Welding
  • MCAW - Metal Core Arc Welding

Deposition Data

Current Diameter Electrical Stickout Voltage Wire Feed Speed
200 A 1.2 mm (.045 in.) 12.7 mm 20 V 533 cm/min (210 in./min)
215 A 1.2 mm (.045 in.) 12.7 mm 21 V 584 cm/min (230 in./min)
234 A 1.2 mm (.045 in.) 12.7 mm 22 V 635 cm/min (250 in./min)
290 A 1.2 mm (.045 in.) 12.7 mm 24 V 762 cm/min (300 in./min)
323 A 1.2 mm (.045 in.) 12.7 mm 24 V 889 cm/min (350 in./min)

Classifications

Grade EC439Nb
Name AWS A5.22

Typical Weld Metal Analysis %

Typical Weld Metal Analysis %
C Cr Mn Nb P S Si Ti
98% Ar - 2% O2
0.02 % 18.60 % 0.70 % 0.50 % 0.01 % 0.02 % 0.51 % 0.25 %
x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : Arcaloy MC18CrCb
ARC MC18CRCB 045X33#PSP 258076850 FIND A DISTRIBUTOR
ARC MC18CRCB 045X600#OMP 258076835 FIND A DISTRIBUTOR
ARCALOY MC18CRCB 045X33# SP 35SB126620 FIND A DISTRIBUTOR
ARCALOY MC18CRCB 045X825# OMP 35SB1294M0 FIND A DISTRIBUTOR
x
x

x

Loading..