Current |
TTW Dist. |
Voltage |
Wire Diameter |
Wire Feed Speed |
75% Ar - 25% CO2
|
430-510 A |
19 mm(3/4 in.) |
32-36 V |
1.6 mm(1/16 in.) |
889-1219 cm/min(350-480 in./min) |
340-430 A |
19 mm(3/4 in.) |
29-32 V |
1.6 mm(1/16 in.) |
635-889 cm/min(250-350 in./min) |
230-340 A |
19 mm(3/4 in.) |
26-29 V |
1.6 mm(1/16 in.) |
381-635 cm/min(150-250 in./min) |
340-410 A |
16 mm(5/8 in.) |
31-36 V |
1.4 mm(.052 in.) |
1016-1346 cm/min(400-530 in./min) |
280-340 A |
16 mm(5/8 in.) |
28-31 V |
1.4 mm(.052 in.) |
762-1016 cm/min(300-400 in./min) |
190-280 A |
16 mm(5/8 in.) |
29-28 V |
1.4 mm(.052 in.) |
457-762 cm/min(180-300 in./min) |
200-260 A |
16 mm(5/8 in.) |
27-28 V |
1.2 mm(.045 in.) |
635-889 cm/min(250-350 in./min) |
260-310 A |
16 mm(5/8 in.) |
28-30 V |
1.2 mm(.045 in.) |
889-1143 cm/min(350-450 in./min) |
230-430 A |
19 mm(3/4 in.) |
24-29 V |
1.6 mm(1/16 in.) |
381-1219 cm/min(150-480 in./min) |
190-420 A |
16 mm(5/8 in.) |
24-32 V |
1.4 mm(.052 in.) |
457-1346 cm/min(180-530 in./min) |
170-390 A |
16 mm(5/8 in.) |
24-32 V |
1.2 mm(.045 in.) |
640-1397 cm/min(250-550 in./min) |
310-360 A |
16 mm(5/8 in.) |
30-33 V |
1.2 mm(.045 in.) |
1143-1397 cm/min(450-550 in./min) |
90% Ar - 10% CO2
|
430-510 A |
19 mm(3/4 in.) |
30-33 V |
1.6 mm(1/16 in.) |
889-1219 cm/min(350-480 in./min) |
370-430 A |
19 mm(3/4 in.) |
28-30 V |
1.6 mm(1/16 in.) |
711-889 cm/min(280-350 in./min) |
230-370 A |
19 mm(3/4 in.) |
24-28 V |
1.6 mm(1/16 in.) |
381-711 cm/min(150-280 in./min) |
370-420 A |
16 mm(5/8 in.) |
30-32 V |
1.4 mm(.052 in.) |
1143-1397 cm/min(450-550 in./min) |
310-370 A |
16 mm(5/8 in.) |
27-30 V |
1.4 mm(.052 in.) |
889-1143 cm/min(350-450 in./min) |
190-310 A |
16 mm(5/8 in.) |
24-27 V |
1.4 mm(.052 in.) |
457-889 cm/min(180-350 in./min) |
330-390 A |
16 mm(5/8 in.) |
29-32 V |
1.2 mm(.045 in.) |
1270-1651 cm/min(500-650 in./min) |
260-330 A |
16 mm(5/8 in.) |
26-29 V |
1.2 mm(.045 in.) |
889-1270 cm/min(350-500 in./min) |
170-260 A |
16 mm(5/8 in.) |
24-26 V |
1.2 mm(.045 in.) |
508-889 cm/min(200-350 in./min) |