Shield-Bright 316L was developed for the welding of Type 316L stainless steel but can be used for other stainless steels including Types 316 and 304L. In a few cases, e.g. nitric acid service, Shield-Bright 316L should not be used to weld 304L. It contains molybdenum which resists pitting corrosion induced by sulphuric and sulphurous acids, chlorides and cellulose solutions. Used widely in the rayon, dye and paper making industries.

BUY NOW


Typical Charpy V-Notch Properties

Impact Value Testing Temperature
as welded c1 shielding gas
60 J -29 degC
26 J -196 degC
as welded c1 shielding gas
60 J -29 degC
26 J -196 degC

Typical Tensile Properties

Condition As Welded As Welded
Shielding Gas M21 Shielding Gas C1 Shielding Gas
Tensile Strength 580 MPa 570 MPa
Yield Strength 450 MPa 442 MPa
Elongation 40 % 53 %

Deposition Data

Current 130-220 A
Deposition Rate 1.9-4.6 kg/h
Diameter 1.2 mm
Voltage 24-29 V
Wire Feed Speed 5.8-14.4 m/min

Classifications

Weld Metal SFA/AWS A5.22 : E316LT1-4
SFA/AWS A5.22 : E316LT1-1
JIS Z 3323 : TS316L-FB1
KS D 3612 : YF 316LC
EN ISO 17633-A : T 19 12 3 L P C1 2
EN ISO 17633-A : T 19 12 3 L P M21 2

Approvals

Approvals ABS E316LT1-1 (C1)
BV 316L (C1)
CE EN 13479
CWB AWS A5.22 E316LT1-1, E316LT1-4
ClassNK KW316LG (C1)
DNV 316L (C1)
KR RW316LG(C) (C1)
LR 316L (C1)
VdTÜV 04834 (M20,M21)
Approvals are based on factory location. Please contact ESAB for more information.

Consumable Characteristics

Alloy Type C Cr Ni Mo
Welding Current DC+

Typical Weld Metal Analysis %

Typical Weld Metal Analysis %
C Cr Mn Mo Ni P S Si
C1 Shielding Gas
- - - 2.60 % - 0.027 % - -
C1 shielding Gas
0.028 % 18.50 % - - 11.8 % - - -
C1 shielding gas
- - 1.10 % - - - 0.010 % 0.80 %
M21 Shielding Gas
0.030 % 18.5 % 1.20 % 2.70 % 12.0 % 0.027 % - 0.90 %
M21 shielding gas
- - - - - - 0.010 % -
x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : Shield-Bright 316L
SB 316L 035X33#SP VP 35FA09982V FIND A DISTRIBUTOR
ES SB316L 1.2X16KG BAWS VP 35FA129840 FIND A DISTRIBUTOR
SB 316L 045X33#SP VP 35FA12982V FIND A DISTRIBUTOR
SB 316L 045X11#SP VP 35FA12560V FIND A DISTRIBUTOR
SB 316L 1/16X33#SP VP 35FA16982V FIND A DISTRIBUTOR
x
x

x

Loading..