Shield-Bright 316L X-tra was developed for the welding Type 316L stainless steel and also can be used for the other stainless steels including Types 316 and 304L. In a few cases, e.g. nitric acid service, Shield-Bright 316L X-tra should not be used to weld 304L. It was designed specifically for applications where the service environment can produce pitting corrosion. Shield-Bright 316L X-tra was developed for welding in the flat position and for horizontal fillet welds with flat to concave beads with excellent slag removal.

BUY NOW


Typical Weld Metal Analysis %

Typical Weld Metal Analysis %
C Cr Mn Mo Ni P S Si
100% CO2
0.026 % 18.5 % 1.47 % 2.70 % 12.0 % 0.024 % 0.006 % 0.46 %
75% Ar - 25% CO2
0.030 % 19.0 % 1.30 % 2.70 % 12.0 % 0.020 % 0.008 % 0.60 %

Approvals

Approvals ABS E316LT0-1 (C1)
CE EN 13479
CWB AWS A5.22 E316LT0-1, E316LT0-4
DNV 316L (C1)
KR RW316LG (C1)
LR 316L S (C1)
VdTÜV 06612
Approvals are based on factory location. Please contact ESAB for more information.

Typical Charpy V-Notch Properties

Impact Value Testing Temperature
45 J(33 ft-lb) -29 degC(-20 degF)
20 J(15 ft-lb) -196 degC(-321 degF)

Classifications

EN ISO 17633-A : T 19 12 3 L R M21 3
EN ISO 17633-A : T 19 12 3 L R C1 3
KS D 3612 : YF 316LC - KR
JIS Z 3323 : TS316L-FB0 - KR
SFA/AWS A5.22 : E316LT0-4
SFA/AWS A5.22 : E316LT0-1

Consumable Characteristics

Welding Current DC+
Alloy Type C Cr Ni Mo

Typical Tensile Properties

As welded As welded
Shielding Gas 75% Ar - 25% CO2 100% CO2
Tensile Strength 580 MPa(84 ksi) 565 MPa(82 ksi)
Yield Strength 450 MPa(65 ksi) 431 MPa(62.5 ksi)
Elongation 36 % 37 %

Deposition Data

Current Deposition Rate Diameter Voltage Wire Feed Speed
150-250 A 2.5-7.0 kg/h(5.5-15.4 lb/h) 1.2 mm(.045 in.) 25-32 V 8.0-16.0 m/min(315-630 in./min)
200-350 A 3.0-7.5 kg/h(6.6-16.5 lb/h) 1.6 mm(1/16 in.) 26-34 V 4.0-11.0 m/min(157.5-433 in./min)
x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : Shield-Bright 316L X-tra
SBX 316L 045x33#SP VP 35FX12982V FIND A DISTRIBUTOR
Shield-Bright 316L X-tra 1.2mm 35FX12248V FIND A DISTRIBUTOR
SBX 316L 1/16x33#SP VP 35FX16982V FIND A DISTRIBUTOR
Shield-Bright 316L X-tra 1.6mm 35FX16120V FIND A DISTRIBUTOR
x
x

x

Loading..