Shield-Bright 309L
Shield-Bright 309L is a rutile cored wire designed for the all-positional welding, except vertical down, of stainless steels to carbon or low alloy steels and for the first layer cladding of carbon and low alloy steels with Ar/15-25%CO2 or CO2 shielding gas.
Typical Charpy V-Notch Properties
Impact Value | Testing Temperature | |||
as welded c1 shielding gas | ||||
55 J | -29 degC | |||
18 J | -196 degC |
Typical Tensile Properties
As welded | As welded | |
Shielding Gas | 75% Ar - 25% CO2 | 100% CO2 |
Tensile Strength | 600 MPa (87 ksi) | 539 MPa (78 ksi) |
Yield Strength | 480 MPa (70 ksi) | 392 MPa (57 ksi) |
Elongation | 35 % | 51 % |
Deposition Data
Current | 130-220 A |
Deposition Rate | 1.9-4.6 kg/h |
Diameter | 1.2 mm |
Voltage | 24-29 V |
Wire Feed Speed | 5.8-14.4 m/min |
Classifications
Classifications |
AWS A5.22 : E309T1-1/T1-4 A5.22 : E309LT1-1/T1-4 |
Approvals
Approvals |
ABS-AWS A5.22 E309LT1-1 ASME II SFA 5.22 E309LT1-1/T1-4 ASME IX F No. 6 AWS A5.22 E309LT1-1/T1-4 CWB AWS A5.22 E309LT1-1, E309LT1-4 G.L.- AWS A5.22 E309LT1-4 MIL-STD-1689 APPLICATIONS-NAVY TUV |
Approvals are based on factory location. Please contact ESAB for more information. |
Consumable Characteristics
Alloy Type | C Cr Ni |
Welding Current | DC+ |
Typical Weld Metal Analysis %
Typical Weld Metal Analysis % | ||||||||||||||
C | Cr | Mn | Ni | P | S | Si | ||||||||
C1 Shielding Gas | ||||||||||||||
0.029 % | - | - | - | 0.024 % | 0.007 % | - | ||||||||
C1 Shielding gas | ||||||||||||||
- | 23.1 % | - | 12.4 % | - | - | - | ||||||||
C1 shielding gas | ||||||||||||||
- | - | 1.10 % | - | - | - | 0.80 % | ||||||||
M21 Shielding Gas | ||||||||||||||
0.030 % | 23.5 % | 1.30 % | 12.5 % | 0.024 % | 0.007 % | 0.90 % |