Shield-Bright 309L X-tra was developed for the welding of stainless steels to carbon or low alloy steels and for the first layer cladding of carbon and low alloy steels. Shield-Bright 309L X-tra was developed for welding in the flat position and for horizontal fillet welds with flat to concave beads with excellent slag removal. For joining thick sections, it is preferred the non-stainless steel be buttered with a layer of Shield-Bright 309L X-tra and the joint completed with Shield-Bright 316L X-tra or 308L X-tra. The service temperature should not exceed approximately 750°F (399°C).

BUY NOW


Typical Charpy V-Notch Properties

Impact Value Testing Temperature
as welded c1 shielding gas
15 J (11 ft-lb) -196 degC (-321 degF)
40 J (30 ft-lb) -29 degC (-20 degF)

Typical Tensile Properties

Condition As Welded As Welded
Shielding Gas M21 Shielding Gas C1 shielding gas
Tensile Strength 600 MPa (87 ksi) 546 MPa (79 ksi)
Yield Strength 480 MPa (70 ksi) 410 MPa (59 ksi)
Elongation 35 % 38 %

Deposition Data

Current Deposition Rate Diameter Voltage Wire Feed Speed
200-350 A 3.0-7.5 kg/h (6-16 lb/h) 1.6 mm (1/16 in.) 26-34 V 4.0-11.0 m/min (157-433 in./min)
150-250 A 2.5-7.0 kg/h (5-15 lb/h) 1.2 mm (0.045 in.) 25-32 V 8.0-16.0 m/min (315-630 in./min)

Classifications

Weld Metal SFA/AWS A5.22 : E309LT0-1
SFA/AWS A5.22 : E309LT0-4
KS D 3612 : YF-309LC
EN ISO 17633-A : T 23 12 L R C1 3
EN ISO 17633-A : T 23 12 L R M21 3
JIS Z 3323 : YF-309LC

Approvals

Approvals ABS E309LT0-1 (C1)
BV 309L (C1)
CCS 309LS (C1)
CE EN 13479
CWB AWS A5.22 E309LT0-1, E309LT0-4
DNV 309L MS (C1)
DNV 309L MS (M21)
VdTÜV 06594
Approvals are based on factory location. Please contact ESAB for more information.

Consumable Characteristics

Alloy Type C Cr Ni
Welding Current DC+

Typical Weld Metal Analysis %

Typical Weld Metal Analysis %
C Cr Mn Ni P S Si
100% CO2
0.032 % 24.50 % 1.46 % 12.8 % 0.021 % 0.004 % 0.66 %
75% Ar - 25% CO2
0.030 % 24.50 % 1.44 % 13.0 % 0.020 % 0.004 % 0.80 %
x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : Shield-Bright 309L X-tra
35CX12982V FIND A DISTRIBUTOR
35CX12248V FIND A DISTRIBUTOR
35CX16982V FIND A DISTRIBUTOR
35CX20982V FIND A DISTRIBUTOR
35CX16248V FIND A DISTRIBUTOR

ESAB EQUIPMENT WARRANTIES ARE VALID ONLY WHEN PURCHASED THROUGH AN ESAB AUTHORIZED DEALERSHIP.

x
x

x

Loading..