Shield-Bright 308L X-tra was designed for welding type 304L stainless steel but can be used for types 301, 302,and 304 steels. It may also be used successfully for welding of types 321 and 347 stainless steel. Service conditions should not exceed an approximate of 750°F (399°C). Shield-Bright 308L X-tra was designed for welding in the flat position and for horizontal fillet welds with flat to concave beads with excellent slag removal.

BUY NOW


Typical Weld Metal Analysis %

Typical Weld Metal Analysis %
C Cr Mn Ni P S Si
100% CO2
0.030 % 19.4 % 1.30 % 9.8 % 0.020 % 0.004 % 0.48 %
75% Ar - 25% CO2
0.022 % 19.6 % 1.40 % 9.9 % 0.020 % 0.004 % 0.90 %

Approvals

Approvals ABS E308LT0-1 (C1)
BV 308L (M21)
CE EN 13479
CWB AWS A5.22 E308LT0-1, E308LT0-4
DNV 308L (C1)
KR RW308LG(C) (C1)
LR 304L S (C1)
VdTÜV 06611
Approvals are based on factory location. Please contact ESAB for more information.

Typical Charpy V-Notch Properties

Impact Value Testing Temperature
40 J(29.5 ft-lb) -29 degC(-20 degF)
24 J(18 ft-lb) -196 degC(-321 degF)

Classifications

EN ISO 17633-A : T 19 9 L R M21 3
EN ISO 17633-A : T 19 9 L R C1 3
KS D 3612 : YF 308LC - KR
JIS Z 3323 : TS308L-FB0 - KR
SFA/AWS A5.22 : E308LT0-4
SFA/AWS A5.22 : E308LT0-1

Consumable Characteristics

Welding Current DC+
Alloy Type C Cr Ni

Typical Tensile Properties

As welded As welded
Shielding Gas 75% Ar - 25% CO2 100% CO2
Tensile Strength 580 MPa(84 ksi) 549 MPa(80 ksi)
Yield Strength 410 MPa(59.5 ksi) 409 MPa(59 ksi)
Elongation 40 % 55 %

Deposition Data

Current Deposition Rate Diameter Voltage Wire Feed Speed
150-250 A 2.5-7.0 kg/h(5.5-15.4 lb/h) 1.2 mm(.045 in.) 25-32 V 8.0-16.0 m/min(315-630 in./min)
200-350 A 3.0-7.5 kg/h(6.6-16.5 lb/h) 1.6 mm(1/16 in.) 26-34 V 4.0-11.0 m/min(157.5-433 in./min)
x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : Shield-Bright 308L X-tra
SBX 308L 045x33#SP VP 35BX12982V FIND A DISTRIBUTOR
Shield-Bright 308L X-tra 1.2mm 35BX12248V FIND A DISTRIBUTOR
SBX 308L 1/16x33#SP VP 35BX16982V FIND A DISTRIBUTOR
x
x

x

Loading..