Shield-Bright 2594

ESAB

Shield-Bright 2594

The following items have been added to your list


x

Shield-Bright 2594 is designed for the welding of 25Cr-9Ni-3Mo-0.2N super duplex stainless steel (UNS S32750, S32760). It has excellent slag removal and bead shape with all position welding for use with Ar/CO2 gas mixtures (M21).

BUY NOW


Industries

  • Chemical Industry
  • Offshore Oil
  • Petrochemical
  • Pipeline
  • Process
  • Pulp and Paper

Welding Process

  • FCAW (Flux Core)

Typical Weld Metal Analysis %

Typical Weld Metal Analysis %
C Cr Cu Mn Mo N Ni P S Si W
0.03 % 25.34 % 0.14 % 0.95 % 3.59 % 0.23 % 9.68 % 0.02 % 0.01 % 0.62 % 0.02 %

Typical Charpy V-Notch Properties

Impact Value Testing Temperature
48 J(35 ft-lb) -29 degC(-20 degF)
44 J(32 ft-lb) -46 degC(-51 degF)

Classifications

EN ISO 17633-A : T 25 9 4 N L P M21 2
SFA/AWS A5.22 : E2594T1-4

Consumable Characteristics

Welding Current DC+
Alloy Type Ni, Cr, Mo, N

Typical Tensile Properties

ElongationTensile Strength Yield Strength
27 %860 MPa (125 ksi)700 MPa (101.5 ksi)

Deposition Data

Wire Feed Speed 8.3-11.5 m/min
Wire Feed Speed 327-453 in./min
Voltage 25-30 V
Diameter 1.2 mm
Diameter .045 in.
Deposition Rate 2.4-4.6 kg/h
Deposition Rate 5.3-10.1 lb/h
Current 150-220 A
x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : Shield-Bright 2594
SB 2594 045X33#SP VP 35HD12982V FIND A DISTRIBUTOR
Shield-Bright 2594 1.2mm15kgVP 35HD12981V FIND A DISTRIBUTOR
Shield-Bright 2594 1.2mm4x5kg 35HD12560V FIND A DISTRIBUTOR
Shield-Bright 2594 1.2mm4x5kg 35HD12561V FIND A DISTRIBUTOR
x
x

x

Loading..