Shield-Bright 2209 was developed for the welding of “2205” duplex stainless steels (UNS S31803, S32205, and J92205). It can also be used for the welding of leaner grades of duplex stainless steels. It has been approved with a 25°C critical pitting temperature and impact toughness at -40°C (-40°F).

BUY NOW


Industries

  • Petrochemical
  • Pipeline
  • Process
  • Pulp and Paper

Welding Process

  • FCAW (Flux Core)

Typical Charpy V-Notch Properties

Impact Value Testing Temperature
as welded 80%ar/20%co2 shielding gas (m21)
55 J (40.5 ft-lb) -20 degC (-4 degF)
45 J (33 ft-lb) -45 degC (-49 degF)
52 J (38 ft-lb) -46 degC (-51 degF)
as welded co2 shielding gas (c1)
50 J (37 ft-lb) -46 degC (-51 degF)

Typical Tensile Properties

As welded As welded
Shielding Gas 80%Ar/20%CO2 Shielding Gas (M21) CO2 Shielding Gas (C1)
Tensile Strength 840 MPa (122 ksi) 800 MPa (116 ksi)
Yield Strength 640 MPa (93 ksi) 650 MPa (94 ksi)
Elongation 27 % 28 %

Deposition Data

Current Deposition Rate Diameter Voltage Wire Feed Speed
130-220 A 1.9-4.6 kg/h (4-10 lb/h) 1.2 mm (0.045 in.) 25-30 V 5.8-14.4 m/min (228-567 in./min)
170-300 A 2.4-5.2 kg/h (5-11 lb/h) 1.6 mm (1/16 in.) 25-29 V 3.9-8.2 m/min (154-323 in./min)

Classifications

Weld Metal SFA/AWS A5.22 : E2209T1-4, E2209T1-1
EN ISO 17633-A : T 22 9 3 N L P C1 2
EN ISO 17633-A : T 22 9 3 N L P M21 2

Approvals

Approvals ABS E2209T1-1 (C1)
BV 2205 (C1)
CCS 2205-S (C1)
CE EN 13479
CWB AWS A5.22 E2209T1-1, E2209T1-4
DNV Duplex (C1)
DNV-GL Duplex (M21)
LR S31803 (C1)
VdTÜV 09123
Approvals are based on factory location. Please contact ESAB for more information.

Consumable Characteristics

Alloy Type Ni, Cr, Mo, N
Welding Current DC+

Typical Weld Metal Analysis %

Typical Weld Metal Analysis %
C Cr Mn Mo N Ni P S Si Si+Fe
C1
0.03 % 23.2 % 1.40 % 3.21 % 0.14 % 8.7 % 0.025 % 0.012 % 0.60 % 40 %
M21
0.03 % 22.5 % 0.90 % 3.2 % 0.16 % 9.2 % 0.025 % 0.012 % 0.35 % 40 %
x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : Shield-Bright 2209
35HC129840 FIND A DISTRIBUTOR
35HC12982V FIND A DISTRIBUTOR
35HC12560V FIND A DISTRIBUTOR
35HC16982V FIND A DISTRIBUTOR

ESAB EQUIPMENT WARRANTIES ARE VALID ONLY WHEN PURCHASED THROUGH AN ESAB AUTHORIZED DEALERSHIP.

x
x

x

Loading..