Cryo-Shield 316L is all position flux cored wire adaptable to a variety of shop and field erection applications. Designed for cryogenic applications where good weld metal toughness is required. Cryo-Shield 316L was developed for the welding of type 316, 316L austenitic stainless steels for the low temperatures. It contains molybdenum which resists pitting corrosion induced by sulphuric and sulphurous acids, chlorides and cellulose solutions. Cryo-Shield 316L was designed titania based slag system with excellent slag removal so they can have high welding speeds because of possible welding in all position in high current area.
Welding Process
- FCAW (Flux Core)
Typical Charpy V-Notch Properties
Impact Value | 40 J |
Shielding Gas | 100% CO2 |
Testing Temperature | -196 °C |
Typical Tensile Properties
Elongation | Shielding Gas | Tensile Strength | Yield Strength |
50 % | 100% CO2 | 529 MPa (77 ksi) | 392 MPa (57 ksi) |
Classifications
Classifications |
JIS Z3323 : TS316L-FB1 AWS A5.22 : E316LT1-1(4) |
Approvals
Approvals |
BV DNV JIS KR LR NK |
Approvals are based on factory location. Please contact ESAB for more information. |
Typical Weld Metal Analysis %
Typical Weld Metal Analysis % | ||||||||||||||
C | Cr | Mn | Mo | Ni | P | S | Si | Si+Fe | ||||||
100% CO2 | ||||||||||||||
0.026 % | 17.5 % | 1.50 % | 2.20 % | 12.4 % | 0.025 % | 0.008 % | 0.70 % | 3-8 % |