Typical Tensile Properties

As welded
Elongation Tensile Strength Yield Strength
42 % 114 ksi 73 ksi

Typical Charpy V-Notch Properties

As welded
Impact Value Testing Temperature
55 ft-lb 0 °C
52 ft-lb -196 °C

Typical Weld Metal Analysis

weld metal analysis
MnMoCNbTiSiNb+TaCrFe
0.24 %8.63 %0.023 %3.8 %0.18 %0.36 %3.57 %21.89 %0.52 %

Classifications: AWS A5.34; ENiCrMo3T1-4; Weld Metal; EN ISO 12153; T Ni 6625 P M 2; Weld Metal

Alloy Type: Ni-Cr-Mo
Welding Current: DC+
x

Typical Tensile Properties

As welded
Elongation Tensile Strength Yield Strength
42 % 114 ksi 73 ksi

Typical Charpy V-Notch Properties

As welded
Impact Value Testing Temperature
55 ft-lb 0 °C
52 ft-lb -196 °C

Typical Weld Metal Analysis

weld metal analysis
MnMoCNbTiSiNb+TaCrFe
0.24 %8.63 %0.023 %3.8 %0.18 %0.36 %3.57 %21.89 %0.52 %

Classifications: AWS A5.34; ENiCrMo3T1-4; Weld Metal; EN ISO 12153; T Ni 6625 P M 2; Weld Metal

Alloy Type: Ni-Cr-Mo
Welding Current: DC+
x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : Shield-Bright NiCrMo-3
SB NICRMO-3 045X33# VP 35ZA12982V FIND A DISTRIBUTOR
SB NICRMO-3 045X11# VP 35ZA1298XX FIND A DISTRIBUTOR
x
×

Find the Closest Distributor

x

x

Loading..