Cryo-Shield Ni9'


Cryo-Shield Ni9


Flux cored wire for welding of 9% Ni steel. Cryo-Shield Ni9 is a gas shielded flux cored wire that can be used for welding in all positions using 100% CO2 shielding gas. This welding material is a Nickel-based with excellent crack resistance and anti-porosity on the weld bead surface.

BUY NOW


Specifications


Typical Tensile Properties

CO2 Shielding gas
Condition Elongation Tensile Strength Yield Strength
As Welded 44 % 730 MPa 440 MPa

Typical Charpy V-Notch Properties

CO2 Shielding gas
Condition Impact Value Testing Temperature
As Welded 65 J -196 °C

Typical Weld Metal Analysis %

CO2 Shielding gas
PMnMoCuCSTiSiNiNb+TaCrFe
0.01 %1.45 %8.15 %0.01 %0.02 %0.002 %0.12 %0.45 %58.5 %3.00 %19.0 %9.0 %

Approvals: ABS; Manufacturer Guarantee

Approvals are based on factory location. Please contact ESAB for more information.


Alloy Type: Ni Cr Mo
Welding Current: DC+
x

Typical Tensile Properties

CO2 Shielding gas
Condition Elongation Tensile Strength Yield Strength
As Welded 44 % 730 MPa 440 MPa

Typical Charpy V-Notch Properties

CO2 Shielding gas
Condition Impact Value Testing Temperature
As Welded 65 J -196 °C

Typical Weld Metal Analysis %

CO2 Shielding gas
PMnMoCuCSTiSiNiNb+TaCrFe
0.01 %1.45 %8.15 %0.01 %0.02 %0.002 %0.12 %0.45 %58.5 %3.00 %19.0 %9.0 %

Approvals: ABS; Manufacturer Guarantee

Approvals are based on factory location. Please contact ESAB for more information.


Alloy Type: Ni Cr Mo
Welding Current: DC+
x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : Cryo-Shield Ni9
Cryo-Shield Ni9 1.2mm 15kg VP 35N912982V FIND A DISTRIBUTOR
x
×

Find the Closest Distributor

x

x

Loading..