Stoody NiCrMo3-T1

Stoody

Stoody NiCrMo3-T1

The following items have been added to your list


x

Stoody NiCrMo3-T1 is a gas shielded flux cored wire that can be used for welding in all positions using argon/CO2 mixtures. The wire possesses excellent weldability and can be used in a wide variety of similar and dissimilar welding and cladding applications. The iron content of the all-weld deposit is kept below 1% for applications requiring enhanced corrosion resistance.

BUY NOW


Features

  • Joining nickel-chromium-molybdenum alloys to UNS N06625. Clad side of joints in steel clad with nickel-chromium-molybdenum weld metal Surfacing steel with nickel-chromium-molybdenum weld metal Joining steels to nickel based alloys Joining 9% nickel steel for cryogenic applications

Industries

  • Petrochemical

Typical Charpy V-Notch Properties

Impact Value Testing Temperature
as welded asme testing using 1 in. thick 9% ni, 3g
77 J (57 ft-lb) -196 degC (-320 degF)
as welded
60 J (44 ft-lb) -196 degC (-320 degF)

Typical Tensile Properties

Condition As Welded As Welded
ASME Testing Using 1 in. Thick 9% Ni, 3G, Cross-Joint
Tensile Strength 725 MPa (105 ksi) 714 MPa (104 ksi)
Yield Strength 470 MPa (68 ksi)
Elongation 38 %

Recommended Welding Parameters

Current 150-200 A
Shielding Gas 75% - Ar/25% - CO2
Voltage 25-27 V
Wire Diameter .045 in.
Wire Diameter 1.2 mm
Wire Feed Speed 290-400 in./min
Wire Feed Speed 735-1000 mm/min

Classifications

Classifications ISO : TNi 6625-14
ENiCrMo3T1-4 :
AWS A5.34/A5.34M : 2018

Typical Weld Metal Analysis %

Typical Weld Metal Analysis %
C Co Cr Fe Mn Mo Nb+Ta Ni P S Si Ti
0.02 % 0.02 % 21.0 % 0.3 % 0.2 % 8.5 % 3.3 % Balance % 0.005 % 0.003 % 0.35 % 0.1 %
x

Part Numbers and Accessories