Shield-Bright NiCrMo-3

The following items have been added to your list


x

A positional rutile wire for the welding of NiCrMoNb alloys, super stainless steels and 9% Ni steels for cryogenic service. It has <1% Fe for higher corrosion resistance.

BUY NOW


Typical Charpy V-Notch Properties

Impact Value Testing Temperature
as welded m21 (ar/15-25% co2)
75 J (56 ft-lb) 0 degC (32 degF)
70 J (52 ft-lb) -196 degC (-321 degF)

Typical Tensile Properties

ConditionElongationShielding GasTensile Strength Yield Strength
As Welded42 %M21 (Ar/15-25% CO2)788 MPa (114 ksi)501 MPa (73 ksi)

Deposition Data

Current 130-210 A
Deposition Rate 4.2-9.3 lb/h
Deposition Rate 1.9-4.2 kg/h
Diameter 0.045 in.
Diameter 1.2 mm
Voltage 23-32 V
Wire Feed Speed 228-543 in./min
Wire Feed Speed 5.8-13.8 m/min

Classifications

Weld Metal AWS A5.34 : ENiCrMo3T1-4
EN ISO 12153 : T Ni 6625 P M21 2

Approvals

Grade 1.2 mm
Society NAKS/HAKC
Approvals are based on factory location. Please contact ESAB for more information.

Consumable Characteristics

Alloy Type Ni-Cr-Mo-Nb
Welding Current DC+

Typical Weld Metal Analysis %

Typical Weld Metal Analysis %
C Cr Cu Fe Mn Mo Nb+Ta P S Si Ti
M21 (Ar/15-25% CO2)
0.02 % 21 % 0.02 % 0.5 % 0.12 % 8.5 % 3.3 % 0.003 % 0.003 % 0.35 % 0.1 %
x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : Shield-Bright NiCrMo-3
SB NICRMO-3 045X33# VP 35ZA12982V FIND A DISTRIBUTOR
SB NICRMO-3 045X11# VP 35ZA1298XX FIND A DISTRIBUTOR
Shield-Bright NiCrMo-3 5kg 12026600 FIND A DISTRIBUTOR