Dual Shield T-75 is a flux cored wire with a basic slag system designed for multiple pass welding and produces excellent properties in both the as welded and stress relieved conditions. The exceptional impact toughness and low sensitivity to cracking makes it an ideal choice for a variety of low and medium carbon steels. The arc characteristics are globular, but can be improved with argon gas mixtures. The weld metal analysis is similar to an E7018 low hydrogen electrode.

BUY NOW


Industries

  • Civil Construction
  • Industrial and General Fabrication
  • Mobile Equipment
  • Railcars

Welding Process

  • FCAW (Flux Core)

Typical Charpy V-Notch Properties

Impact Value Testing Temperature
as welded 100% co2
95 J (70 ft-lb) -40 degC (-40 degF)
as welded 75% ar - 25% co2
75 J (55 ft-lb) -40 degC (-40 degF)

Typical Tensile Properties

Condition As Welded As Welded
Reduction in Area 66 % 65 %
Shielding Gas 75% Ar - 25% CO2 100% CO2
Tensile Strength 595 MPa (86 ksi) 565 MPa (82 ksi)
Yield Strength 505 MPa (73 ksi) 495 MPa (72 ksi)
Elongation 29 % 28 %

Recommended Welding Parameters

Current TTW Dist. Voltage Wire Diameter Wire Feed Speed
75% Ar - 25% CO2
140-190 A 19-25.4 mm (3/4-1 in.) 19-28 V 1.2 mm (.045 in.) 635-889 cm/min (250-350 in./min)
240-265 A 19-25.4 mm (3/4-1 in.) 29-30 V 1.2 mm (.045 in.) 1143-1397 cm/min (450-550 in./min)
300 A 19-25.4 mm (3/4-1 in.) 32 V 1.2 mm (.045 in.) 1651 cm/min (650 in./min)
220-280 A 19-25.4 mm (3/4-1 in.) 29-30 V 1.6 mm (1/16 in.) 457-635 cm/min (180-250 in./min)
280-380 A 25.4-31.75 mm (1-1.25 in.) 31-32 V 1.6 mm (1/16 in.) 635-1016 cm/min (250-400 in./min)
240-370 A 25.4-31.75 mm (1-1.25 in.) 30-32 V 2.4 mm (3/32 in.) 254-508 cm/min (100-200 in./min)
370-460 A 31.75-38 mm (1.25-1.5 in.) 32-33 V 2.4 mm (3/32 in.) 508-813 cm/min (200-320 in./min)

Deposition Data

Current Deposition Rate Diameter Deposition Efficiency (%) TTW Dist. Voltage Wire Feed Speed
100% CO2
450 A 8.0 kg/h (17.6 lb/h) 2.4 mm (3/32 in.) 85 % 25.4 mm (1 in.) 32 V 551 cm/min (217 in./min)
475 A 9.1 kg/h (20 lb/h) 2.4 mm (3/32 in.) 87 % 25.4 mm (1 in.) 32 V 622 cm/min (245 in./min)
500 A 10.3 kg/h (22.8 lb/h) 2.4 mm (3/32 in.) 89 % 25.4 mm (1 in.) 32 V 686 cm/min (270 in./min)

Classifications

Classifications ASME SFA 5.36 :
ASME SFA 5.20 :
AWS A5.36 : E70T5-M21-CS1-H4
AWS A5.36 : E70T5-C1A4-CS1-H4
AWS A5.20 : E70T-5C-JH4/T-5M-JH

Approvals

Approvals ABS
DNV-GL (3/32")
LR
QPL-24403/1 MIL-70T-5C (3/32")
Approvals are based on factory location. Please contact ESAB for more information.

Typical Weld Metal Analysis %

Typical Weld Metal Analysis %
C Mn P S Si
100% CO2
0.04 % 1.50 % 0.006 % 0.010 % 0.60 %
75% Ar - 25% CO2
0.04 % 1.70 % 0.004 % 0.011 % 0.70 %
x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : Dual Shield T-75
245020128 FIND A DISTRIBUTOR
245020417 FIND A DISTRIBUTOR
423006006 FIND A DISTRIBUTOR
243006004 FIND A DISTRIBUTOR

ESAB EQUIPMENT WARRANTIES ARE VALID ONLY WHEN PURCHASED THROUGH AN ESAB AUTHORIZED DEALERSHIP.

x
x

x

Loading..