Dual Shield II 712X

The following items have been added to your list


x

Dual Shield II 712X is an all-position flux cored wire intended for applications requiring outstanding weld metal toughness. This X Series wire, in combination with 75% Argon/25% CO2 shielding gas, can produce Charpy V-Notch impact results of more than 40 ft-lb (68 J) at -60°F (-51°C) and Crack Tip Opening Displacement (CTOD) results of more than 20 mils (0.5 mm) at -40°F (-40°C). Dual Shield II 712X also provides the smooth arc and low spatter levels characteristic of Dual Shield flux cored wires. Applications include off-shore oil components, shipbuilding and heavy equipment where exceptional Charpy impact/low temperature toughness is required.

BUY NOW


Industries

  • Offshore Oil
  • Ship/Barge Building
  • Heavy Equipment

Welding Process

  • FCAW (Flux Core)

Typical Charpy V-Notch Properties

as welded 75% ar - 25% co2

Typical Tensile Properties

ConditionElongationShielding GasTensile Strength Yield Strength
As Welded28 %75% Ar - 25% CO2570 MPa (83 ksi)540 MPa (78 ksi)

Classifications

Classifications ASME SFA 5.36 :
ASME SFA 5.20 :
AWS A5.36 : E71T1-M21A6-CS2-H8
AWS A5.20 : E71T-1MJH8/T-9MJH8/T-12MJH8

Approvals

Approvals ABS
CWB W48 E491T-12MJ-H8
DNV-GL
LR
Approvals are based on factory location. Please contact ESAB for more information.

Typical Weld Metal Analysis %

Typical Weld Metal Analysis %
C Mn P S Si
75% Ar - 25% CO2
0.05 % 1.1 % 0.009 % 0.010 % 0.3 %
x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : Dual Shield II 712X
245019757 Find a distributor
245019765 Find a distributor
245019773 Find a distributor
245019781 Find a distributor

ESAB EQUIPMENT WARRANTIES ARE VALID ONLY WHEN PURCHASED THROUGH AN ESAB AUTHORIZED DEALERSHIP.

x
x

x

Loading..