Dual Shield II 70 Ultra

ESAB

Dual Shield II 70 Ultra

The following items have been added to your list


x

Dual Shield II 70 Ultra is an all-position flux cored wire that displays exceptional impact properties when used with 75% Ar/25% CO2. The improved properties qualify this wire to the Navys "HY" classification. The "Ultra" series produces smoother arc characteristics and lower welding fumes. Dual Shield II 70 Ultra was developed to join low and medium carbon steel. The Military classification allows Dual Shield II 70 Ultra to be used for attaching steels of less than 81 ksi (560 MPa) yield to HY-80 and HY-100. Commercial applications include construction, shipbuilding, railcar, and heavy equipment industries.

BUY NOW


Industries

  • Bridge Construction
  • Civil Construction
  • Industrial and General Fabrication
  • Mobile Equipment
  • Railcars
  • Ship/Barge Building

Welding Process

  • FCAW (Flux Core)

Typical Weld Metal Analysis %

Typical Weld Metal Analysis %
C Mn P S Si
75% Ar - 25% CO2
0.03 % 1.1 % 0.008 % 0.004 % 0.45 %

Approvals

Society CL
Society DB
Society BV
Society ABS
Society LR
Grade CSA W48 491T-1M-H8
Society CWB
Society DNL-GL
Grade 71T-1-HYM
Society MIL
Grade 71T-1M
Society MIL
Approvals are based on factory location. Please contact ESAB for more information.

Typical Charpy V-Notch Properties

Condition Impact Value (met) Testing Temperature
75% Ar - 25% CO2
As Welded 108 J(80 ft-lb) -40 degC(-40 degF)
As Welded 159 J(117 ft-lb) -18 degC(0 degF)
As Welded 149 J(110 ft-lb) -29 degC(-20 degF)

Classifications

Name ASME SFA 5.36
Name ASME SFA 5.20
Grade E71T1-M21A4-CS2-H8
Name AWS A5.36
Grade E71T-1M-Jh8/T-9M-JH8/T12-M-JH8
Name AWS A5.20

Typical Tensile Properties

ConditionElongationReduction in AreaShielding GasTensile Strength (imp)Yield Strength (imp)
As Welded29 %75 %75% Ar - 25% CO2560 MPa (81 ksi)490 MPa (72 ksi)

Recommended Welding Parameters

Current TTW Dist. Voltage Wire Diameter Wire Feed Speed
75% Ar - 25% CO2
285-340 A 19-25.4 mm(3/4-1 in.) 27-30 V 1.6 mm(1/16 in.) 508-762 cm/min(200-300 in./min)
340-400 A 25.4-31.8 mm(1-1.25 in.) 28-32 V 1.6 mm(1/16 in.) 762-1066.8 cm/min(300-420 in./min)
185-285 A 15.8-19 mm(5/8-3/4 in.) 24-28 V 1.6 mm(1/16 in.) 279.4-508 cm/min(110-200 in./min)
295-355 A 19-25.4 mm(3/4-1 in.) 27-31 V 1.4 mm(.052 in.) 863.6-1193.8 cm/min(340-470 in./min)
250-295 A 15.8-19 mm(5/8-3/4 in.) 25-29 V 1.4 mm(.052 in.) 584.2-863.6 cm/min(230-340 in./min)
135-250 A 12.7-15.8 mm(1/2-5/8 in.) 22-26 V 1.4 mm(.052 in.) 279.4-584.2 cm/min(110-230 in./min)
225-265 A 19-25.4 mm(3/4-1 in.) 27-29 V 1.2 mm(.045 in.) 965.2-1320.8 cm/min(380-520 in./min)
200-225 A 12.7-19 mm(1/2-3/4 in.) 24-27 V 1.2 mm(.045 in.) 660.4-965.2 cm/min(260-380 in./min)
130-200 A 9.5-12.7 mm(3/8-1/2 in.) 22-26 V 1.2 mm(.045 in.) 381-660.4 cm/min(150-260 in./min)
160-215 A 15.8 mm(5/8 in.) 24.5-28 V 0.9 mm(.035 in.) 1016-1905 cm/min(400-750 in./min)
110-140 A 15.8 mm(5/8 in.) 22-24 V 0.9 mm(.035 in.) 635-1016 cm/min(250-400 in./min)

Deposition Data

Current Deposition Rate Diameter Efficiency (%) Voltage Wire Feed Speed
75% Ar - 25% CO2
110 A 1.32 kg/h(2.9 lb/h) 0.9 mm(.035 in.) 84.00 % 22 V 635 cm/min(250 in./min)
140 A 2.13 kg/h(4.7 lb/h) 0.9 mm(.035 in.) 85.00 % 24 V 1016 cm/min(400 in./min)
160 A 2.54 kg/h(5.6 lb/h) 0.9 mm(.035 in.) 85.00 % 24.5 V 1206 cm/min(475 in./min)
180 A 2.94 kg/h(6.5 lb/h) 0.9 mm(.035 in.) 86.00 % 25.5 V 1394 cm/min(550 in./min)
215 A 4.08 kg/h(9.0 lb/h) 0.9 mm(.035 in.) 87.00 % 28 V 1905 cm/min(750 in./min)
145 A 1.79 kg/h(3.94 lb/h) 1.2 mm(.045 in.) 86.15 % 22 V 508 cm/min(200 in./min)
210 A 2.72 kg/h(5.99 lb/h) 1.2 mm(.045 in.) 85.51 % 23 V 762 cm/min(300 in./min)
247 A 3.68 kg/h(8.10 lb/h) 1.2 mm(.045 in.) 87.55 % 24.5 V 1016 cm/min(400 in./min)
275 A 4.33 kg/h(9.52 lb/h) 1.2 mm(.045 in.) 82.08 % 26 V 1270 cm/min(500 in./min)
150 A 1.82 kg/h(4.01 lb/h) 1.4 mm(.052 in.) 83.25 % 21 V 381 cm/min(150 in./min)
75/25
192 A 2.48 kg/h(5.44 lb/h) 1.4 mm(.052 in.) 84.71 % 22 V 508 cm/min(200 in./min)
262 A 3.69 kg/h(8.12 lb/h) 1.4 mm(.052 in.) 85.48 % 23.5 V 762 cm/min(300 in./min)
308 A 4.97 kg/h(10.92 lb/h) 1.4 mm(.052 in.) 86.31 % 25 V 1016 cm/min(400 in./min)
203 A 2.56 kg/h(5.63 lb/h) 1.6 mm(1/16 in.) 87.15 % 23 V 381 cm/min(150 in./min)
298 A 4.25 kg/h(9.33 lb/h) 1.6 mm(1/16 in.) 87.56 % 24.5 V 635 cm/min(250 in./min)
340 A 5.05 kg/h(11.10 lb/h) 1.6 mm(1/16 in.) 87.68 % 25.5 V 762 cm/min(300 in./min)
375 A 6.02 kg/h(13.24 lb/h) 1.6 mm(1/16 in.) 88.35 % 26 V 889 cm/min(350 in./min)
408 A 6.59 kg/h(14.49 lb/h) 1.6 mm(1/16 in.) 85.66 % 27.5 V 1016 cm/min(400 in./min)
x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : Dual Shield II 70 Ultra
DS II 70 ULT .9X15KG AWS 425013752 FIND A DISTRIBUTOR
DS II 70 ULT .9X4.5KG PSP 425013745 FIND A DISTRIBUTOR
DS II 70 ULT 035X10#FR HS 245014626-34 FIND A DISTRIBUTOR
DS II 70 ULT 035X10#PSP 245013743 FIND A DISTRIBUTOR
DS II 70 ULT 035X10#PSP 245013743-03 FIND A DISTRIBUTOR
DS II 70 ULT 035X33#PSP 245013750 FIND A DISTRIBUTOR
DS II 70 ULT 035X33#PSP 245013750-01 FIND A DISTRIBUTOR
DS II 70 ULT 035X33#PSP 245013750-03 FIND A DISTRIBUTOR
DS II 70 ULT 035X33#PSP 245013750-23 FIND A DISTRIBUTOR
DS II 70 ULT 035X33#PSP 245013750-38 FIND A DISTRIBUTOR
DS II 70 ULT 045X10#PSP 245013370-05 FIND A DISTRIBUTOR
DS II 70 ULT 045X10#PSP 245013370-23 FIND A DISTRIBUTOR
DS II 70 ULT 045X10#PSP 245015821-05 FIND A DISTRIBUTOR
DS II 70 ULT 045X10#PSP HS 245013420-05 FIND A DISTRIBUTOR
DS II 70 ULT 045X15#PSP 245014709 FIND A DISTRIBUTOR
DS II 70 ULT 045X15#PSP 245014709-03 FIND A DISTRIBUTOR
DS II 70 ULT 045X25#FR HS 245014600-34 FIND A DISTRIBUTOR
DS II 70 ULT 045X33#PSP 245013313 FIND A DISTRIBUTOR
DS II 70 ULT 045X33#PSP 245013313-01 FIND A DISTRIBUTOR
DS II 70 ULT 045X33#PSP 245013313-02 FIND A DISTRIBUTOR
DS II 70 ULT 045X33#PSP 245013313-03 FIND A DISTRIBUTOR
DS II 70 ULT 045X33#PSP VP 245013453 FIND A DISTRIBUTOR
DS II 70 ULT 045X60#CL 245013388-55 FIND A DISTRIBUTOR
DS II 70 ULT 052X10#PSP 245013396-03 FIND A DISTRIBUTOR
DS II 70 ULT 052X10#PSP 245013396-23 FIND A DISTRIBUTOR
DS II 70 ULT 052X15#PSP 245014857 FIND A DISTRIBUTOR
DS II 70 ULT 052X15#PSP 245014857-03 FIND A DISTRIBUTOR
DS II 70 ULT 052X33#PSP 245013321 FIND A DISTRIBUTOR
DS II 70 ULT 1.2X15KG AWS 425013315 FIND A DISTRIBUTOR
DS II 70 ULT 1.2X15KG AWS EU 425014651 FIND A DISTRIBUTOR
DS II 70 ULT 1.2X4.54KG PSP 425013372 FIND A DISTRIBUTOR
DS II 70 ULT 1.2X4.54KG PSP 425813375 FIND A DISTRIBUTOR
DS II 70 ULT 1.6X15KG AWS 425013331 FIND A DISTRIBUTOR
DS II 70 ULT 1.6X4.54KG PSP 425013364 FIND A DISTRIBUTOR
DS II 70 ULT 1/16X10#PSP 245013362-03 FIND A DISTRIBUTOR
DS II 70 ULT 1/16X10#PSP 245013362-23 FIND A DISTRIBUTOR
DS II 70 ULT 1/16X15#PSP 245014808 FIND A DISTRIBUTOR
DS II 70 ULT 1/16X15#PSP 245014808-03 FIND A DISTRIBUTOR
DS II 70 ULT 1/16X25#HS 245016019-05 FIND A DISTRIBUTOR
DS II 70 ULT 1/16X33#PSP 245013339 FIND A DISTRIBUTOR
DS II 70 ULT 1/16X33#PSP 245013339-03 FIND A DISTRIBUTOR
DS II 70 ULT 1/16X60#CL 245013354 FIND A DISTRIBUTOR
DS II 70 ULT 1/16X60#CL 245013354-55 FIND A DISTRIBUTOR