Dual Shield 710X-M

ESAB

Dual Shield 710X-M

The following items have been added to your list


x

Dual Shield 710X-M provides outstanding operator appeal with an easily controlled arc, improved operation at both lower and higher current levels, minimal spatter and easily removed slag. Dual Shield 710X-M is designed to be used with 75/25 Argon CO2 gas mix.

BUY NOW


Industries

  • Barges
  • Civil Construction
  • Industrial and General Fabrication
  • Railcars
  • Ship/Barge Building
  • Light Equipment

Welding Process

  • FCAW (Flux Core)

Typical Charpy V-Notch Properties

Impact Value Testing Temperature
as welded 75% ar - 25% co2
97 J (72 ft-lb) -18 degC (0 degF)
76 J (56 ft-lb) -29 degC (-20 degF)

Typical Tensile Properties

ConditionElongationShielding GasTensile Strength Yield Strength
As Welded29 %75% Ar - 25% CO2570 MPa (83 ksi)510 MPa (74 ksi)

Deposition Data

Current Deposition Rate Diameter Deposition Efficiency (%) TTW Dist. Voltage Wire Feed Speed
75% Ar - 25% CO2
290 A 4.05 kg/h (8.92 lb/h) 1.2 mm (.045 in.) 87 % 25.4 mm (1 in.) 1143 cm/min (450 in./min)
270 A 3.70 kg/h (8.17 lb/h) 1.2 mm (.045 in.) 87 % 25.4 mm (1 in.) 29 V 1016 cm/min (400 in./min)
250 A 3.21 kg/h (7.08 lb/h) 1.2 mm (.045 in.) 86 % 25.4 mm (1 in.) 29 V 889 cm/min (350 in./min)
230 A 2.66 kg/h (5.86 lb/h) 1.2 mm (.045 in.) 84 % 19 mm (3/4 in.) 27 V 762 cm/min (300 in./min)
210 A 2.22 kg/h (4.90 lb/h) 1.2 mm (.045 in.) 86 % 19 mm (3/4 in.) 27 V 635 cm/min (250 in./min)
190 A 1.75 kg/h (3.85 lb/h) 1.2 mm (.045 in.) 85.5 % 12.7 mm (1/2 in.) 26 V 508 cm/min (200 in./min)
150 A 1.28 kg/h (2.82 lb/h) 1.2 mm (.045 in.) 79 % 12.7 mm (1/2 in.) 26 V 381 cm/min (150 in./min)
370 A 5.55 kg/h (12.23 lb/h) 1.4 mm (.052 in.) 86 % 25.4 mm (1 in.) 32 V 1270 cm/min (500 in./min)
360 A 5.01 kg/h (11.05 lb/h) 1.4 mm (.052 in.) 87 % 25.4 mm (1 in.) 32 V 1143 cm/min (450 in./min)
350 A 4.44 kg/h (9.80 lb/h) 1.4 mm (.052 in.) 86 % 25.4 mm (1 in.) 32 V 1016 cm/min (400 in./min)
340 A 3.92 kg/h (8.65 lb/h) 1.4 mm (.052 in.) 86 % 19 mm (3/4 in.) 30 V 889 cm/min (350 in./min)
310 A 3.33 kg/h (7.35 lb/h) 1.4 mm (.052 in.) 86 % 19 mm (3/4 in.) 30 V 762 cm/min (300 in./min)
260 A 2.72 kg/h (6.00 lb/h) 1.4 mm (.052 in.) 86 % 19 mm (3/4 in.) 30 V 635 cm/min (250 in./min)
220 A 2.20 kg/h (4.86 lb/h) 1.4 mm (.052 in.) 84.5 % 15.8 mm (5/8 in.) 28 V 508 cm/min (200 in./min)
190 A 1.66 kg/h (3.66 lb/h) 1.4 mm (.052 in.) 83 % 15.8 mm (5/8 in.) 28 V 381 cm/min (150 in./min)
480 A 7.33 kg/h (16.17 lb/h) 1.6 mm (1/16 in.) 87 % 31.75 mm (1 1/4 in.) 32 V 1143 cm/min (450 in./min)
430 A 6.49 kg/h (14.33 lb/h) 1.6 mm (1/16 in.) 87 % 31.75 mm (1 1/4 in.) 32 V 1016 cm/min (400 in./min)
420 A 5.72 kg/h (12.63 lb/h) 1.6 mm (1/16 in.) 86.5 % 31.75 mm (1 1/4 in.) 32 V 889 cm/min (350 in./min)
360 A 4.85 kg/h (10.70 lb/h) 1.6 mm (1/16 in.) 86 % 25.4 mm (1 in.) 30 V 635 cm/min (250 in./min)
360 A 4.04 kg/h (8.90 lb/h) 1.6 mm (1/16 in.) 86 % 25.4 mm (1 in.) 30 V 635 cm/min (250 in./min)
300 A 3.21 kg/h (7.08 lb/h) 1.6 mm (1/16 in.) 85.5 % 19 mm (3/4 in.) 28 V 508 cm/min (200 in./min)
250 A 2.37 kg/h (5.23 lb/h) 1.6 mm (1/16 in.) 85 % 19 mm (3/4 in.) 28 V 381 cm/min (150 in./min)

Classifications

Classifications ASME SFA 5.36 :
ASME SFA 5.20 :
AWS A5.36 : E71T1-M21A4-CS1-DH8
AWS A5.20 : E71T-1MD-H8/T-9MD-H8

Approvals

Approvals ABS
CWB CSA W48 E491T-9M-H8
DNV-GL
LR
MIL-E-24403A 71T-1M
Seismic Certified "D"
Approvals are based on factory location. Please contact ESAB for more information.

Typical Weld Metal Analysis %

Typical Weld Metal Analysis %
C Mn P S Si
75% Ar - 25% CO2
0.04 % 1.3 % 0.012 % 0.008 % 0.5 %
x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : Dual Shield 710X-M
DS 710X-M 045X33#AWS 245019807
DS 710X-M 045X60#CL 245019245 FIND A DISTRIBUTOR
DS 710X-M 045X600#OMP 245019237 FIND A DISTRIBUTOR
DS 710X-M 052X33#AWS 245019815 FIND A DISTRIBUTOR
DS 710X-M 052X60#CL 245019880 FIND A DISTRIBUTOR
DS 710X-M 052X600#OMP 2/PLT 245019849 FIND A DISTRIBUTOR
DS 710X-M 1/16X33#AWS 245019823 FIND A DISTRIBUTOR
DS 710X-M 1/16X50#CL 245019872 FIND A DISTRIBUTOR
DS 710X-M 1/16X60#CL 245019831 FIND A DISTRIBUTOR
DS 710X-M 1/16X600#OMP 245019864 FIND A DISTRIBUTOR
x
x

x

Loading..