Typical Charpy V-Notch Properties

Impact Value Testing Temperature
as welded
123 J (91 ft-lb) -29 degC (-20 degF)
94 J (69 ft-lb) -40 degC (-40 degF)
89 J (66 ft-lb) -46 degC (-50 degF)
stress relieved
115 J (85 ft-lb) 8 hr 620 degC (1150 degF) -29 degC (-20 degF)
86 J (63 ft-lb) 8 hr 620 degC (1150 degF) -40 degC (-40 degF)
76 J (56 ft-lb) 8 hr 620 degC (1150 degF) -46 degC (-50 degF)

Typical Tensile Properties

Condition Stress Relieved As Welded
Tensile Strength 498 MPa (72 ksi) 510 MPa (74 ksi)
Yield Strength 405 MPa (59 ksi) 425 MPa (62 ksi)
Elongation 33 % 32 %
Testing Time 8 hr
Testing Temperature 620 degC (1150 degF)

Deposition Data

Current Diameter TTW Dist. Voltage
280-460 A 1.6 mm (1/16 in.) 20-25 mm (0.75-1 in.) 26-36 V
160-280 A 1.6 mm (1/16 in.) 13-25 mm (0.5-1 in.) 24-28 V
280-390 A 1.4 mm (.052 in.) 20-25 mm (0.75-1 in.) 24-34 V
150-280 A 1.4 mm (.052 in.) 13-25 mm (0.5-1 in.) 22-28 V
270-330 A 1.2 mm (.045 in.) 20-25 mm (0.75-1 in.) 24-34 V
140-270 A 1.2 mm (.045 in.) 13-25 mm (0.5-1 in.) 22-28 V

Classifications

Classifications SFA/AWS A5.36 : E71T1-M21-P5-CS2 H4
SFA/AWS A5.36 : E71T1-M21-A5-CS2 H4
SFA/AWS A5.20 : E71T-9MJH4/T-12MJH4

Approvals

Approvals CWB CSA W48: Class E491T-9MJ-H4, E491T-12MJ-H4
LR 5Y40S(H5)
Approvals are based on factory location. Please contact ESAB for more information.

Consumable Characteristics

Alloy Type C Mn Ni
Diffusible Hydrogen 3.8
Welding Current DC+

Typical Weld Metal Analysis %

Typical Weld Metal Analysis %
C Mn Ni P S Si
0.03 % 1.40 % 0.45 % 0.013 % 0.005 % 0.41 %
x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : Dual Shield 7100SRM
243006376 FIND A DISTRIBUTOR

ESAB EQUIPMENT WARRANTIES ARE VALID ONLY WHEN PURCHASED THROUGH AN ESAB AUTHORIZED DEALERSHIP.

x
x

x

Loading..