Dual Shield 7100 LC

ESAB

Dual Shield 7100 LC

The following items have been added to your list


x

Dual Shield 7100 LC provides outstanding operator appeal with its easily controlled arc, improved operation at lower current levels, minimal spatter and easily removed slag. Dual Shield 7100 LC can be used with CO2 or 75% Ar/25% CO2 shielding, however pure CO2 is recommended in applications where restraint is high.

BUY NOW


Industries

  • Bridge Construction
  • Civil Construction
  • Industrial and General Fabrication
  • Mobile Equipment
  • Process
  • Railcars
  • Ship/Barge Building

Welding Process

  • FCAW (Flux Core)

Typical Charpy V-Notch Properties

Impact Value Testing Temperature
as welded 100% co2
92 J (68 ft-lb) -18 degC (0 degF)
56 J (41 ft-lb) -29 degC (-20 degF)
as welded 75% ar - 25% co2
61 J (50 ft-lb) -18 degC (0 degF)
42 J (31 ft-lb) -29 degC (-20 degF)

Typical Tensile Properties

Condition As Welded As Welded
Reduction in Area 52 % 64 %
Shielding Gas 100% CO2 75% Ar - 25% CO2
Tensile Strength 560 MPa (81 ksi) 621 MPa (90 ksi)
Yield Strength 565 MPa (73 ksi) 572 MPa (83 ksi)
Elongation 23 % 26 %

Recommended Welding Parameters

Current TTW Dist. Voltage Wire Diameter Wire Feed Speed
100% CO2
290-415 A 25.4-31.75 mm (1-1.25 in.) 28-32 V 1.6 mm (1/16 in.) 1016-1270 cm/min (400-500 in./min)
245-345 A 19-25.4 mm (3/4-1 in.) 27-30 V 1.6 mm (1/16 in.) 673-1016 cm/min (265-400 in./min)
250-350 A 19-25.4 mm (3/4-1 in.) 29-31 V 1.4 mm (.052 in.) 1016-1524 cm/min (400-600 in./min)
180-265 A 19-25.4 mm (3/4-1 in.) 26-30 V 1.2 mm (.045 in.) 889-1397 cm/min (350-550 in./min)
175-230 A 12.7-19 mm (1/2-3/4 in.) 25-27 V 1.2 mm (.045 in.) 737-889 cm/min (290-350 in./min)
135-205 A 9.5-12.7 mm (3/8-1/2 in.) 23-26 V 1.2 mm (.045 in.) 432-737 cm/min (170-290 in./min)
125-235 A 12.7-16 mm (1/2-5/8 in.) 23-26 V 1.4 mm (.052 in.) 330-711 cm/min (130-280 in./min)
215-290 A 16-19 mm (5/8-3/4 in.) 25-29 V 1.4 mm (.052 in.) 711-1016 cm/min (280-400 in./min)
165-270 A 16-19 mm (5/8-3/4 in.) 25-28 V 1.6 mm (1/16 in.) 343-673 cm/min (135-265 in./min)
75% Ar - 25% CO2
285-400 A 25.4-31.75 mm (1-1.25 in.) 28-32 V 1.6 mm (1/16 in.) 813-1168 cm/min (320-460 in./min)
250-340 A 19-25.4 mm (3/4-1 in.) 27-30 V 1.6 mm (1/16 in.) 610-813 cm/min (240-320 in./min)
185-265 A 19-25.4 mm (3/4-1 in.) 27-29 V 1.2 mm (.045 in.) 775-1194 cm/min (305-470 in./min)
130-200 A 9.5-12.7 mm (3/8-1/2 in.) 22-26 V 1.2 mm (.045 in.) 356-610 cm/min (140-240 in./min)
185-285 A 16-19 mm (5/8-3/4 in.) 24-28 V 1.6 mm (1/16 in.) 356-610 cm/min (140-240 in./min)
245-355 A 19-25.4 mm (3/4-1 in.) 28-32 V 1.4 mm (.052 in.) 940-1372 cm/min (370-540 in./min)
225-295 A 16-19 mm (5/8-3/4 in.) 27-30 V 1.4 mm (.052 in.) 686-940 cm/min (270-370 in./min)
135-250 A 12.7-16 mm (1/2-5/8 in.) 24-28 V 1.4 mm (.052 in.) 317.5-686 cm/min (125-270 in./min)
165-225 A 12.7-19 mm (1/2-3/4 in.) 24-27 V 1.2 mm (.045 in.) 610-775 cm/min (240-305 in./min)

Deposition Data

Current Deposition Rate Diameter Deposition Efficiency (%) Voltage Wire Feed Speed
100% CO2
145 A 1.6 kg/h (3.6 lb/h) 1.2 mm (.045 in.) 81.2 % 24.5 V 508 cm/min (200 in./min)
190 A 2.5 kg/h (5.4 lb/h) 1.2 mm (.045 in.) 81.4 % 26 V 762 cm/min (300 in./min)
235 A 3.3 kg/h (7.3 lb/h) 1.2 mm (.045 in.) 82.5 % 27.5 V 1016 cm/min (400 in./min)
265 A 4.2 kg/h (9.3 lb/h) 1.2 mm (.045 in.) 82.8 % 29 V 1270 cm/min (500 in./min)
145 A 1.5 kg/h (3.4 lb/h) 1.4 mm (.052 in.) 74.3 % 25 V 381 cm/min (150 in./min)
180 A 2.0 kg/h (4.5 lb/h) 1.4 mm (.052 in.) 74.6 % 25.5 V 508 cm/min (200 in./min)
230 A 5.5 kg/h (12.2 lb/h) 1.4 mm (.052 in.) 82.3 % 29.5 V 1270 cm/min (500 in./min)
235 A 3.2 kg/h (7.0 lb/h) 1.4 mm (.052 in.) 78.2 % 27.5 V 762 cm/min (300 in./min)
285 A 4.4 kg/h (9.8 lb/h) 1.4 mm (.052 in.) 81.3 % 28.5 V 1016 cm/min (400 in./min)
370 A 6.7 kg/h (14.7 lb/h) 1.4 mm (.052 in.) 82.7 % 30.2 V 1524 cm/min (600 in./min)
195 A 2.0 kg/h (4.5 lb/h) 1.6 mm (1/16 in.) 73.7 % 24.5 V 381 cm/min (150 in./min)
285 A 3.7 kg/h (8.1 lb/h) 1.6 mm (1/16 in.) 79.4 % 26 V 635 cm/min (250 in./min)
320 A 4.4 kg/h (9.7 lb/h) 1.6 mm (1/16 in.) 79.9 % 28 V 762 cm/min (300 in./min)
345 A 5.2 kg/h (11.5 lb/h) 1.6 mm (1/16 in.) 80.7 % 30 V 889 cm/min (350 in./min)
385 A 6.1 kg/h (13.4 lb/h) 1.6 mm (1/16 in.) 82.6 % 32 V 1016 cm/min (400 in./min)
445 A 7.6 kg/h (16.7 lb/h) 1.6 mm (1/16 in.) 82.8 % 32.5 V 1270 cm/min (500 in./min)

Classifications

Classifications ASME SFA 5.36 :
ASME SFA 5.20 :
AWS A5.36 : E71T1-M21A2-CS1-H8
AWS A5.36 : E71T1-C1A4-CS1-DH8
AWS A5.20 : E71T-1C-DH8/T-1MH8/T-9C-DH8/T-9MH8

Approvals

Approvals ABS
CWB CSA W48 E491T-9-H8, E491T-9M-H8
DNV-GL
LR
Seismic Certified "D"
Approvals are based on factory location. Please contact ESAB for more information.

Typical Weld Metal Analysis %

Typical Weld Metal Analysis %
C Mn P S Si
100% CO2
0.03 % 1.2 % 0.010 % 0.010 % 0.5 %
75% Ar - 25% CO2
0.03 % 1.4 % 0.010 % 0.010 % 0.6 %
x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : Dual Shield 7100 LC
DS 7100 LC 045X33#AWS 248000937 FIND A DISTRIBUTOR
DS 7100 LC 045X60#CL 248000895 FIND A DISTRIBUTOR
DS 7100 LC 052X15#PSP 248001091 FIND A DISTRIBUTOR
DS 7100 LC 052X33#AWS 248000960 FIND A DISTRIBUTOR
DS 7100 LC 052X60#CL 248001042 FIND A DISTRIBUTOR
DS 7100 LC 1/16X33#AWS 248000903 FIND A DISTRIBUTOR
DS 7100 LC 1/16X33#AWS BK 248000978 FIND A DISTRIBUTOR
DS 7100 LC 1/16X33#PSP 248001067 FIND A DISTRIBUTOR
DS 7100 LC 1/16X60#CL 248000929 FIND A DISTRIBUTOR
DS 7100 LC 1/16X600#OMP 248001083 FIND A DISTRIBUTOR
x
x

x

Loading..