Dual Shield 700X is a high deposition, deep penetration wire for joining of heavy structural steel components. Designed for flat and horizontal position welding using CO2 shielding gas, this X Series wire provides high deposition rates, high efficiency and excellent performance. The bead contour, smooth ripple and slag chemistry allow easy slag removal even in narrow groves.

BUY NOW


Industries

  • Agricultural Equipment
  • Mobile Equipment
  • Heavy Equipment
  • Large Components

Welding Process

  • FCAW (Flux Core)

Typical Weld Metal Analysis %

Typical Weld Metal Analysis %
C P S
100% CO2
0.035 % 0.011 % 0.015 %

Approvals

Approvals A.B.S.- 2SA,2YSA
ASME SFA 5.20
AWS A5.20 E70T-1CH8/T-9CH8
CERTIFIED BY C.W.B.- CSA W48
DNV III YMS
L.R. - 3S,3YS
Approvals are based on factory location. Please contact ESAB for more information.

Typical Charpy V-Notch Properties

Impact Value Testing Temperature
66 J(49 ft-lb) -18 degC(0 degF)
45 J(33 ft-lb) -29 degC(-20 degF)

Classifications

Name AWS A5.20
Grade E70T-1CH8/T-9CH8

Typical Tensile Properties

ConditionElongationShielding GasTensile Strength Yield Strength
As Welded29 %100% CO2600 MPa (87 ksi)545 MPa (79 ksi)

Recommended Welding Parameters

Current TTW Dist. Voltage Wire Diameter Wire Feed Speed
100% CO2
180-460 A 19-25.4 mm(3/4-1 in.) 25-34 V 1.6 mm(1/16 in.) 343-1270 mm/min(135-500 in./min)
290-610 A 25.4-38 mm(1-1.5 in.) 26-34 V 2.4 mm(3/32 in.) 254-825.5 mm/min(100-325 in./min)

Deposition Data

Current Deposition Rate Diameter Efficiency (%) TTW Dist. Voltage Wire Feed Speed
100% CO2
149 A 1.3 kg/h(2.8 lb/h) 1.6 mm(1/16 in.) 80 % 19 mm(3/4 in.) 23 V 254 cm/min(100 in./min)
168 A 1.6 kg/h(3.5 lb/h) 1.6 mm(1/16 in.) 80 % 19 mm(3/4 in.) 24 V 305 cm/min(120 in./min)
187 A 1.9 kg/h(4.2 lb/h) 1.6 mm(1/16 in.) 80 % 19 mm(3/4 in.) 24 V 356 cm/min(140 in./min)
205 A 2.2 kg/h(4.9 lb/h) 1.6 mm(1/16 in.) 80 % 19 mm(3/4 in.) 25 V 406 cm/min(160 in./min)
223 A 2.5 kg/h(5.6 lb/h) 1.6 mm(1/16 in.) 80 % 19 mm(3/4 in.) 25 V 457 cm/min(180 in./min)
240 A 2.9 kg/h(6.3 lb/h) 1.6 mm(1/16 in.) 80 % 19 mm(3/4 in.) 25 V 508 cm/min(200 in./min)
257 A 3.2 kg/h(7.0 lb/h) 1.6 mm(1/16 in.) 81 % 19 mm(3/4 in.) 26 V 559 cm/min(220 in./min)
273 A 3.5 kg/h(7.7 lb/h) 1.6 mm(1/16 in.) 81 % 19 mm(3/4 in.) 26 V 610 cm/min(240 in./min)
289 A 3.8 kg/h(8.4 lb/h) 1.6 mm(1/16 in.) 81 % 19 mm(3/4 in.) 26 V 660 cm/min(260 in./min)
290 A 5.8 kg/h(12.7 lb/h) 2.4 mm(3/32 in.) 86.9 % 25.4 mm(1 in.) 27 V 381 cm/min(150 in./min)
350 A 7.7 kg/h(16.9 lb/h) 2.4 mm(3/32 in.) 86.3 % 25.4 mm(1 in.) 28 V 508 cm/min(200 in./min)
410 A 9.6 kg/h(21.1 lb/h) 2.4 mm(3/32 in.) 86 % 25.4 mm(1 in.) 29 V 635 cm/min(250 in./min)
475 A 11.3 kg/h(25.0 lb/h) 2.4 mm(3/32 in.) 84.8 % 25.4 mm(1 in.) 32 V 762 cm/min(300 in./min)
x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : Dual Shield 700X
DS 700X 1/16X33#AWS 245019500 FIND A DISTRIBUTOR
DS 700X 1/16X60#CL 245019526 FIND A DISTRIBUTOR
DS 700X 3/32X60#CL 245019518 FIND A DISTRIBUTOR
DS 700X 3/32X850#RL 245019534 FIND A DISTRIBUTOR
x
x

x

Loading..