Pipeweld 71T-1

ESAB

Pipeweld 71T-1

The following items have been added to your list


x

An all-positional rutile cored wire for pipe welding. The weld metal has a minimum yield strength of 420 MPa with CO2 shielding gas and 460 MPa with Ar/CO2 mixed gas.

BUY NOW


Typical Charpy V-Notch Properties

Impact Value Testing Temperature
as welded c1 shielding gas
65 J (48 ft-lb) -30 degC (-22 degF)
as welded m21 shielding gas
70 J (52 ft-lb) -40 degC (-40 degF)

Typical Tensile Properties

Condition As Welded As Welded
Shielding Gas C1 Shielding gas M21 Shielding gas
Tensile Strength 585 MPa (85 ksi) 601 MPa (87 ksi)
Yield Strength 495 MPa (72 ksi) 535 MPa (78 ksi)
Elongation 25 % 25 %

Deposition Data

Current Deposition Rate Diameter TTW Dist. Voltage Wire Feed Speed
150-350 A 2.1-7.5 kg/h (4.6-16.5 lb/h) 1.2 mm (.045 in.) 23-35 V 5.8-20.7 m/min (2.3-8.1 ft/min)
205-230 A - 1.2 mm (.045 in.) 12.7-19 mm (1/2-3/4 in.) 25-27 V 660-965 cm/min (260-380 in./min)
135-205 A - 1.2 mm (.045 in.) 9.5-12.7 mm (3/8-1/2 in.) 23-26 V 381-660 cm/min (150-260 in./min)
230-265 A - 1.2 mm (.045 in.) 19-25.4 mm (3/4-1 in.) 26-30 V 965-1321 cm/min (380-520 in./min)

Classifications

Weld Metal SFA/AWS A5.20 : E71T-1M H8
EN ISO 17632-A : T 46 4 P M21 1 H5
EN ISO 17632-A : T 42 3 P C1 1 H5
SFA/AWS A5.20 : E71T-1C H4

Consumable Characteristics

Alloy Type Non alloy
Welding Current DC+

Typical Weld Metal Analysis %

Typical Weld Metal Analysis %
C Mn Si
M21 Shielding gas
- - 0.63 %
M21 shielding gas
0.059 % 1.33 % -
x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : Pipeweld 71T-1
350312560V FIND A DISTRIBUTOR

ESAB EQUIPMENT WARRANTIES ARE VALID ONLY WHEN PURCHASED THROUGH AN ESAB AUTHORIZED DEALERSHIP.

x
x

x

Loading..