Typical Charpy V-Notch Properties

As Welded
Impact Value 44 ft-lb
Impact Value 60 J
Shielding Gas M21 shielding gas
Testing Temperature -40 °F
Testing Temperature -40 °C

Typical Tensile Properties

ConditionElongationShielding GasTensile Strength Yield Strength
As Welded19 %M21 shielding gas840 MPa (122 ksi)761 MPa (110 ksi)

Deposition Data

Current Deposition Rate Diameter TTW Dist. Voltage Wire Feed Speed
150-350 A 2.1-7.5 kg/h (4.6-16.5 lb/h) 1.2 mm (.045 in.) 21-32 V 5.6-19.8 m/min (2.2-7.8|ft/min in./min)
205-230 A 1.2 mm (.045 in.) 12.7-19 mm (1/2-3/4 in.) 25-27 V 660-965 cm/min (260-380 in./min)
135-205 A 1.2 mm (.045 in.) 9.5-12.7 mm (3/8-1/2 in.) 23-26 V 381-660 cm/min (150-260 in./min)
230-265 A 1.2 mm (.045 in.) 19-25.4 mm (3/4-1 in.) 26-30 V 965-1321 cm/min (380-520 in./min)

Classifications

Weld Metal SFA/AWS A5.36 : E111T1-M21A4-K3-H4
SFA/AWS A5.29 : E111T1-K3MJ-H4
EN ISO 18276-A : T 69 4 2NiMo P M21 2 H5

Consumable Characteristics

Alloy Type Low Alloy (Ni Mo)
Shielding Gas M21 (EN ISO 14175)
Welding Current DC+

Typical Weld Metal Analysis %

Typical Weld Metal Analysis %
C Mn Mo Ni Si
0.055 % 1.21 % 0.4 % 2.3 % 0.39 %
x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : Pipeweld 111T-1
350412560V Find a distributor

ESAB EQUIPMENT WARRANTIES ARE VALID ONLY WHEN PURCHASED THROUGH AN ESAB AUTHORIZED DEALERSHIP.

x
x

x

Loading..