An all-positional rutile cored wire for pipe welding of steels with a minimum strength of 610 MPa, for use with Ar/CO2 mixed gas.

BUY NOW


Typical Charpy V-Notch Properties

As Welded
Impact Value 70 J
Shielding Gas M21 Shielding gas
Testing Temperature -40 °C

Typical Tensile Properties

ConditionElongationShielding GasTensile Strength Yield Strength
As Welded25 %M21 Shielding gas709 MPa654 MPa

Deposition Data

Current Deposition Rate Diameter TTW Dist. Voltage Wire Feed Speed
100-300 A 1.3-5.8 kg/h (2.9-12.8 lb/h) 1.2 mm (.045 in.) 21-32 V 3.2-14.5 m/min (1.3-5.7 in./min)
205-230 A 1.2 mm (.045 in.) 12.7-19 mm (1/2-3/4 in.) 25-27 V 660-965 cm/min (260-380 in./min)
135-205 A 1.2 mm (.045 in.) 9.5-12.7 mm (3/8-1/2 in.) 23-26 V 381-660 cm/min (150-260 in./min)
230-265 A 1.2 mm (.045 in.) 19-25.4 mm (3/4-1 in.) 26-30 V 965-1321 cm/min (380-520 in./min)

Classifications

Weld Metal SFA/AWS A5.36 : E101T1-M21A4-G
EN ISO 18276-A : T 62 4 Mn1Ni P M 2 H5

Consumable Characteristics

Alloy Type Low alloy
Welding Current DC+

Typical Weld Metal Analysis %

Typical Weld Metal Analysis %
C Mn Mo Ni Si
M21 Shielding gas
- 1.54 % 0.15 % 0.97 % -
M21 shielding gas
0.06 % - - - 0.40 %
x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : Pipeweld 101T-1
Pipeweld 101T-1 1.2mm 16kg VP 350212773V FIND A DISTRIBUTOR
Pipeweld 101T-1 1.2mm 4x5kg VP 350212560V FIND A DISTRIBUTOR
x
x

x

Loading..